Songhan Plastic Technology Co.,Ltd.
 POLYMER SEARCH

Polymer Property : Limiting Pressure Velocity = 0.0701 MPa-m/sec Product List

Mechanical Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Mechanical Properties Metric English Comments
Limiting Pressure Velocity 0.0701 MPa-m/sec
2000 psi-ft/min
4:1 safety factor; QTM 55007
Quadrant EPP Armor-X™ Non-Marring, Elastomer Polymeric Blend (ASTM Product Data Sheet)
Limiting Pressure Velocity 0.0701 MPa-m/sec
2000 psi-ft/min
4:1 safety factor applied; QTM 55010
Quadrant EPP Durapro® Truck Liners (ASTM Product Data Sheet)
Limiting Pressure Velocity 0.0701 MPa-m/sec
2000 psi-ft/min
4:1 safety factor; QTM 55007
Quadrant EPP TIVAR® Dockguard - UHMW-PE - Black UV Stabilized UHMW-PE (ASTM Product Data Sheet)
Limiting Pressure Velocity 0.0701 MPa-m/sec
2000 psi-ft/min
4:1 safety factor; QTM 55007
Quadrant EPP TIVAR® Extended Wear UHMW-PE, Premium Glass-filled, Partially Cross-linked (ASTM Product Data Sheet)
Limiting Pressure Velocity 0.0701 MPa-m/sec
2000 psi-ft/min
4:1 safety factor; QTM 55007
Quadrant EPP TIVAR® SuperPlus UHMW-PE, Glass-filled Cross-linked & Heat Stabilized Extreme Wear Resistant (ASTM Product Data Sheet)
Limiting Pressure Velocity 0.0701 - 0.590 MPa-m/sec
2000 - 16800 psi-ft/min
Average value: 0.167 MPa-m/sec Grade Count:8
Overview of materials for Acetal Copolymer, Unreinforced
This property data is a summary of similar materials in the MatWeb database for the category "Acetal Copolymer, Unreinforced". Each property range of values reported is minimum and maximum values of..
Limiting Pressure Velocity 0.0701 MPa-m/sec
2000 psi-ft/min
4:1 safety factor; QTM 55007
Quadrant EPP Quicksilver® UHMW-PE Premium Truck Lining (ASTM Product Data Sheet)
Limiting Pressure Velocity 0.0701 MPa-m/sec
2000 psi-ft/min
4:1 safety factor; QTM 55007
Quadrant EPP Semitron® ESd 225, Extruded, Static Dissipative Acetal (ASTM Product Data Sheet)
Copyright © lookpolymers.com All Rights Reserved