Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Tensile Strength, Yield | 275 MPa @Strain 0.200 %, Temperature -80.0 °C |
39900 psi @Strain 0.200 %, Temperature -112 °F |
EN min.; EN 10002-5 |
Outokumpu 4401 Cr-Ni-Mo Austenitic Stainless Steel General purpose steel with excellent corrosion resistance, particularly in the presence of halides.Applications: FiltersBraiding for hydraulic hosesShaftsFastenersMarine componentsAvailable in hot r.. |
|||
Tensile Strength, Yield | 275 MPa @Strain 0.200 %, Temperature -80.0 °C |
39900 psi @Strain 0.200 %, Temperature -112 °F |
EN min.; EN 10002-5 |
Outokumpu 4404 Cr-Ni-Mo Austenitic Stainless Steel General purpose steel with excellent corrosion resistance, particularly in the presence of halides.Applications: FiltersBraiding for hydraulic hosesShaftsFastenersMarine componentsAvailable in hot r.. |
|||
Tensile Strength, Yield | 275 MPa @Strain 0.200 %, Temperature -80.0 °C |
39900 psi @Strain 0.200 %, Temperature -112 °F |
EN min.; EN 10002-5 |
Outokumpu 4432 Cr-Ni-Mo Austenitic Stainless Steel General purpose steel with excellent corrosion resistance, particularly in the presence of halides.Applications: FiltersBraiding for hydraulic hosesShaftsFastenersMarine componentsAvailable in hot r.. |
|||
Tensile Strength, Yield | 275 MPa @Strain 0.200 %, Temperature -80.0 °C |
39900 psi @Strain 0.200 %, Temperature -112 °F |
EN min.; EN 10002-5 |
Outokumpu 4435 Cr-Ni-Mo Austenitic Stainless Steel Applications: Wet corrosion resistance and general service.Available in hot rolled plate (Quarto), hot rolled strip/sheet (CPP), cold rolled strip/sheet, cold rolled narrow strip, bar, and rod forms.. |
|||
Tensile Strength, Yield | 275 MPa @Strain 0.200 %, Temperature -80.0 °C |
39900 psi @Strain 0.200 %, Temperature -112 °F |
EN min.; EN 10002-5 |
Outokumpu 4436 Cr-Ni-Mo Austenitic Stainless Steel General purpose steel with excellent corrosion resistance, particularly in the presence of halides.Applications: FiltersBraiding for hydraulic hosesShaftsFastenersMarine componentsAvailable in hot r.. |
|||
Tensile Strength, Yield | 275 MPa @Strain 0.200 %, Temperature -80.0 °C |
39900 psi @Strain 0.200 %, Temperature -112 °F |
EN min.; EN 10002-5 |
Outokumpu 4571 Cr-Ni-Mo Austenitic Stainless Steel Very good corrosion resistance, weldable, and resistant to sensitization.Available in hot rolled plate (Quarto), hot rolled strip/sheet (CPP), cold rolled strip/sheet, cold rolled narrow strip, bar,.. |
|||
Tensile Strength, Yield | 275 MPa @Strain 0.200 % |
39900 psi @Strain 0.200 % |
Outokumpu Typical,Hot Rolled Plate (Quarto); EN 10002-1 |
Outokumpu 4841 High Temperature Austenitic Stainless Steel Variant of 1.4845 with an increased silicon content which enhances the steel's resistance to oxidation/corrosion but has also made it more susceptible to embrittlement.Applications: Heat and creep r.. |
|||
Tensile Strength, Yield | 275 MPa @Temperature -50.0 °C |
39900 psi @Temperature -58.0 °F |
ASTM D638 |
Gharda Chemicals G-PAEKâ„¢ 1230CF Ultra High Performance PEK Polymer Product Details: Ultra High Performance Thermoplastic material, 30% carbon fiber reinforced in Poly Aryl Ether Ketone, semi-crystalline granules suitable for injection molding, easy flow, Black in .. |
|||
Tensile Strength, Yield | >= 275 MPa @Strain 1.00 % |
>= 39900 psi @Strain 1.00 % |
|
Industeel URANUS® B6 Multipurpose Austenitic Stainless Steel with PREN = 34 Description: URANUS® B6 (904L) is a multipurpose 20 Cr - 4.3 Mo high corrosion resistance austenitic stainless steel developed 40 years ago by CLI. The UR B6N is alloyed with nitrogen (~ 0.13%) t.. |
|||
Tensile Strength, Yield | >= 275 MPa @Strain 1.00 % |
>= 39900 psi @Strain 1.00 % |
|
Industeel URANUS® B6 N Multipurpose Austenitic Stainless Steel with PREN = 36 Description: URANUS® B6 (904L) is a multipurpose 20 Cr - 4.3 Mo high corrosion resistance austenitic stainless steel developed 40 years ago by CLI. The UR B6N is alloyed with nitrogen (~ 0.13%) t.. |
|||
Tensile Strength, Yield | 275 MPa @Strain 0.200 %, Temperature 650 °C |
39900 psi @Strain 0.200 %, Temperature 1200 °F |
|
Haynes 75 Nickel Alloy Sheet, Annealed at 1925°F (1050°C) Haynes alloy 75 is a solution-strengthened nickel-chromium alloy with moderate strength to 1200°F (650°C). It is principally used in low stress elevated temperature applications requiring reas.. |
|||
Tensile Strength, Yield | 275 MPa @Thickness 3.20 mm, Temperature 538 °C |
39900 psi @Thickness 0.126 in, Temperature 1000 °F |
0.2% offset |
Haynes Hastelloy® C-4 alloy, sheet, aged 100 hours at 899°C Nickel-chromium-molybdenum alloy with outstanding high-temperature stability as evidenced by high ductility and corrosion resistance even after aging in the 1200 to 1900°F (649 to 1038°C) range. T.. |
|||
Tensile Strength, Yield | 275 MPa @Thickness 4.00 mm, Temperature 204 °C |
39900 psi @Thickness 0.157 in, Temperature 399 °F |
0.2% offset |
Haynes Hastelloy® C-4 alloy, sheet, heat treated at 1066°C, rapid quenched Nickel-chromium-molybdenum alloy with outstanding high-temperature stability as evidenced by high ductility and corrosion resistance even after aging in the 1200 to 1900°F (649 to 1038°C) range. T.. |
|||
Tensile Strength, Yield | 275 - 296 MPa @Strain 0.200 % |
39900 - 42900 psi @Strain 0.200 % |
Plate, Hot-rolled & Solution Annealed |
Special Metals INCOLOY® alloy 803 Fe-Ni-Cr Alloy INCOLOY® alloy 803 (UNS S35045), an iron-nickel-chromium alloy, is designed for use in petrochemical, chemical and thermal processing applications. The nickel and chromium contents of alloy 803 ar.. |
|||
Tensile Strength, Yield | 275 - 310 MPa @Strain 0.200 % |
39900 - 45000 psi @Strain 0.200 % |
Tubing, Cold-drawn & Solution Annealed |
Special Metals INCOLOY® alloy 803 Fe-Ni-Cr Alloy INCOLOY® alloy 803 (UNS S35045), an iron-nickel-chromium alloy, is designed for use in petrochemical, chemical and thermal processing applications. The nickel and chromium contents of alloy 803 ar.. |
|||
Tensile Strength, Yield | 275 - 331 MPa @Strain 0.200 % |
39900 - 48000 psi @Strain 0.200 % |
Sheet, Cold-rolled & Solution Annealed |