Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Tensile Strength, Yield | 275 - 296 MPa @Strain 0.200 % |
39900 - 42900 psi @Strain 0.200 % |
Plate, Hot-rolled & Solution Annealed |
Special Metals INCOLOY® alloy 803 Fe-Ni-Cr Alloy INCOLOY® alloy 803 (UNS S35045), an iron-nickel-chromium alloy, is designed for use in petrochemical, chemical and thermal processing applications. The nickel and chromium contents of alloy 803 ar.. |