Mechanical Properties Metric English Comments
Tensile Strength, Yield 159 MPa

@Thickness 1.57 mm
23000 psi

@Thickness 0.0620 in
LW; ASTM D638
Industrial Laminates/Norplex NP193P Synthetic Fabric
Description: 17 oz. aramid and "soft glass" fibers are combined to make a fabric that is stronger than pure aramid and less abrasive than glass fabrics. This material is impregnated with a high temp..
Tensile Strength, Yield 159 MPa

@Thickness 8.00 mm
23000 psi

@Thickness 0.315 in
LW
Industrial Laminates/Norplex SP525M (WaveMax 5000) Glass Fabric
Description: Non-woven substrate combined with high temperature, static dissipative epoxy resin. Superior machining properties. Capable of producing thin walls with high strength for finely machined..
Tensile Strength, Yield 159 MPa

@Strain 0.200 %,
Temperature 191 °C
23000 psi

@Strain 0.200 %,
Temperature 375 °F
Typical
Magnesium Elektron Elektron® 21 Magnesium Casting Alloy
Fully heat treatable alloy for use up to 400°F. Excellent corrosion resistance and castability. Cast products possess a fine-grained microstructure and pressure tightness. Easily machined. Usual ..