Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Tensile Strength, Yield | 159 MPa @Thickness 1.57 mm |
23000 psi @Thickness 0.0620 in |
LW; ASTM D638 |
Industrial Laminates/Norplex NP193P Synthetic Fabric Description: 17 oz. aramid and "soft glass" fibers are combined to make a fabric that is stronger than pure aramid and less abrasive than glass fabrics. This material is impregnated with a high temp.. |
|||
Tensile Strength, Yield | 159 MPa @Thickness 8.00 mm |
23000 psi @Thickness 0.315 in |
LW |
Industrial Laminates/Norplex SP525M (WaveMax 5000) Glass Fabric Description: Non-woven substrate combined with high temperature, static dissipative epoxy resin. Superior machining properties. Capable of producing thin walls with high strength for finely machined.. |
|||
Tensile Strength, Yield | 159 MPa @Temperature 316 °C |
23100 psi @Temperature 601 °F |
|
ATI Allegheny Ludlum 316Ti Austenitic Stainless Steel Characteristics:excellent resistance to general corrosion, excellent resistance to pitting/crevice corrosion, resistant to sensitization, better creep stress-rupture and tensile strength at elevated.. |
|||
Tensile Strength, Yield | 159 MPa @Strain 0.200 %, Temperature 191 °C |
23000 psi @Strain 0.200 %, Temperature 375 °F |
Typical |
Magnesium Elektron Elektron® 21 Magnesium Casting Alloy Fully heat treatable alloy for use up to 400°F. Excellent corrosion resistance and castability. Cast products possess a fine-grained microstructure and pressure tightness. Easily machined. Usual .. |