Mechanical Properties Metric English Comments
Tensile Strength, Yield 119 MPa

@Strain 0.200 %,
Temperature 500 °C
17300 psi

@Strain 0.200 %,
Temperature 932 °F
EN min.; EN 10002-5
Outokumpu 4311 Cr-Ni Austenitic Stainless Steel
Applications: Wet corrosion resistance and general service.Available in hot rolled plate (Quarto), hot rolled strip/sheet (CPP), cold rolled strip/sheet, cold rolled narrow strip, bar, and rod forms..
Tensile Strength, Yield 119 MPa

@Strain 0.200 %,
Temperature 300 °C
17300 psi

@Strain 0.200 %,
Temperature 572 °F
EN min.; EN 10002-5
Outokumpu 4435 Cr-Ni-Mo Austenitic Stainless Steel
Applications: Wet corrosion resistance and general service.Available in hot rolled plate (Quarto), hot rolled strip/sheet (CPP), cold rolled strip/sheet, cold rolled narrow strip, bar, and rod forms..
Tensile Strength, Yield 119 MPa

@Strain 0.200 %,
Temperature 500 °C
17300 psi

@Strain 0.200 %,
Temperature 932 °F
EN min.; EN 10002-5
Outokumpu 4541 Cr-Ni Austenitic Stainless Steel
Good corrosion resistance and weldable. Resistant to sensitization.Applications: Welded screensFurnace beltsCatalytic converter meshAvailable in hot rolled plate (Quarto), hot rolled strip/sheet (C..
Tensile Strength, Yield >= 119 MPa

@Temperature 300 °C
>= 17300 psi

@Temperature 572 °F
PEAK Werkstoff DISPAL S263 Aluminum Alloy, AlSi25Cu3Fe3Ni3MgCoTi, Condition T6
Excellent properties:abrasive stabilityhigh stiffness (E-modulus)resistance even at high temperaturesgood grindabilityPEAK DISPAL materials allow the manufacturing of pistons for highest operational..
Tensile Strength, Yield 119 MPa

@Temperature -40.0 °C
17300 psi

@Temperature -40.0 °F
ASTM D638
BASF Ultramid® 8270 HS BK 102 PA6 (Conditioned)
Description: Ultramid 8270 HS BK-102 is a thermally modified pigmented black, PA6 blow molding compound exhibiting exceptional toughness and melt strength ideally suited for blow molding, profile ex..