Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Tensile Strength, Yield | 119 MPa @Strain 0.200 %, Temperature 500 °C |
17300 psi @Strain 0.200 %, Temperature 932 °F |
EN min.; EN 10002-5 |
Outokumpu 4311 Cr-Ni Austenitic Stainless Steel Applications: Wet corrosion resistance and general service.Available in hot rolled plate (Quarto), hot rolled strip/sheet (CPP), cold rolled strip/sheet, cold rolled narrow strip, bar, and rod forms.. |
|||
Tensile Strength, Yield | 119 MPa @Strain 0.200 %, Temperature 300 °C |
17300 psi @Strain 0.200 %, Temperature 572 °F |
EN min.; EN 10002-5 |
Outokumpu 4435 Cr-Ni-Mo Austenitic Stainless Steel Applications: Wet corrosion resistance and general service.Available in hot rolled plate (Quarto), hot rolled strip/sheet (CPP), cold rolled strip/sheet, cold rolled narrow strip, bar, and rod forms.. |
|||
Tensile Strength, Yield | 119 MPa @Strain 0.200 %, Temperature 500 °C |
17300 psi @Strain 0.200 %, Temperature 932 °F |
EN min.; EN 10002-5 |
Outokumpu 4541 Cr-Ni Austenitic Stainless Steel Good corrosion resistance and weldable. Resistant to sensitization.Applications: Welded screensFurnace beltsCatalytic converter meshAvailable in hot rolled plate (Quarto), hot rolled strip/sheet (C.. |
|||
Tensile Strength, Yield | >= 119 MPa @Temperature 300 °C |
>= 17300 psi @Temperature 572 °F |
|
PEAK Werkstoff DISPAL S263 Aluminum Alloy, AlSi25Cu3Fe3Ni3MgCoTi, Condition T6 Excellent properties:abrasive stabilityhigh stiffness (E-modulus)resistance even at high temperaturesgood grindabilityPEAK DISPAL materials allow the manufacturing of pistons for highest operational.. |
|||
Tensile Strength, Yield | 119 MPa @Temperature -40.0 °C |
17300 psi @Temperature -40.0 °F |
ASTM D638 |
BASF Ultramid® 8270 HS BK 102 PA6 (Conditioned) Description: Ultramid 8270 HS BK-102 is a thermally modified pigmented black, PA6 blow molding compound exhibiting exceptional toughness and melt strength ideally suited for blow molding, profile ex.. |