Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Tensile Strength, Yield | 900 - 1100 MPa @Strain 0.2 % |
131000 - 160000 psi @Strain 0.2 % |
as built |
EOS MS1 Maraging Steel for DMLS 3D Printing EOS Maraging Steel MS1 is a steel powder which has been optimized especially for processing on EOSINT M 270 systems. This steel has very good mechanical properties, and is easily heat-treatable us.. |
|||
Tensile Strength, Yield | 1000 - 1100 MPa @Strain 0.2 % |
145000 - 160000 psi @Strain 0.2 % |
as built, XY direction |
EOS PH1 Precipitation Hardening Stainless Steel for DMLS 3D Printing EOS Stainless Steel PH1 is a stainless steel powder which has been optimized especially for processing on EOSINT M 270 systems. This stainless steel prototyping material is tough and resistant to .. |