Polymer Property : Tensile Strength, Yield = 145000 psi Product List

Mechanical Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Mechanical Properties Metric English Comments
Tensile Strength, Yield 1000 - 1100 MPa

@Strain 0.2 %
145000 - 160000 psi

@Strain 0.2 %
as built, XY direction
EOS PH1 Precipitation Hardening Stainless Steel for DMLS 3D Printing
EOS Stainless Steel PH1 is a stainless steel powder which has been optimized especially for processing on EOSINT M 270 systems. This stainless steel prototyping material is tough and resistant to ..
Tensile Strength, Yield 1000 MPa

@Strain 0.200 %
145000 psi

@Strain 0.200 %
Tempering Temperature- 600°F
Crucible Steel 422 Stainless Steel
Crucible 422 is a hardenable martensitic stainless steel which is being widely used for high temperatures up to 1200°F. It has excellent creep-rupture properties in the range of 600/1200°F and is..
Tensile Strength, Yield 1000 - 1380 MPa

@Temperature 20.0 °C
145000 - 200000 psi

@Temperature 68.0 °F
varies with heat treatment
Bohler-Uddeholm BÖHLER W302 SUPERIOR® Premium H13 Tool Steel
A premium grade H13 hot work tool steel featuring:Very good toughness properties meeting the requirements of NADCA 207-97, and the superior quality levels of NADCA 207-2003Very good heat checking re..
Tensile Strength, Yield 1000 - 1380 MPa

@Strain 0.200 %,
Temperature 20.0 °C
145000 - 200000 psi

@Strain 0.200 %,
Temperature 68.0 °F
Bohler-Uddeholm BÖHLER W303 ISODISC® Hot Work Tool Steel
Description: Hot work tool steel featuring excellent hot tensile properties, high retention of hardness, good toughness and resistance to heat checking, admits water cooling. BOHLER W303 is also ava..
Tensile Strength, Yield 1000 - 1380 MPa

@Temperature 20.0 °C
145000 - 200000 psi

@Temperature 68.0 °F
varies with heat treatment
Bohler-Uddeholm BÖHLER W302 ISOBLOC® H13 hot work tool steel
Properties:Hot work tool steel featuring excellent hot tensile properties, high hot wear resistance, adequate toughness and heat checking resistance, adequate toughness and heat checking; admits wat..