Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Tensile Strength, Yield | 1000 - 1100 MPa @Strain 0.2 % |
145000 - 160000 psi @Strain 0.2 % |
as built, XY direction |
EOS PH1 Precipitation Hardening Stainless Steel for DMLS 3D Printing EOS Stainless Steel PH1 is a stainless steel powder which has been optimized especially for processing on EOSINT M 270 systems. This stainless steel prototyping material is tough and resistant to .. |
|||
Tensile Strength, Yield | 1000 MPa @Strain 0.200 % |
145000 psi @Strain 0.200 % |
Tempering Temperature- 600°F |
Crucible Steel 422 Stainless Steel Crucible 422 is a hardenable martensitic stainless steel which is being widely used for high temperatures up to 1200°F. It has excellent creep-rupture properties in the range of 600/1200°F and is.. |
|||
Tensile Strength, Yield | 1000 - 1380 MPa @Temperature 20.0 °C |
145000 - 200000 psi @Temperature 68.0 °F |
varies with heat treatment |
Bohler-Uddeholm BÖHLER W302 SUPERIOR® Premium H13 Tool Steel A premium grade H13 hot work tool steel featuring:Very good toughness properties meeting the requirements of NADCA 207-97, and the superior quality levels of NADCA 207-2003Very good heat checking re.. |
|||
Tensile Strength, Yield | 1000 - 1380 MPa @Strain 0.200 %, Temperature 20.0 °C |
145000 - 200000 psi @Strain 0.200 %, Temperature 68.0 °F |
|
Bohler-Uddeholm BÖHLER W303 ISODISC® Hot Work Tool Steel Description: Hot work tool steel featuring excellent hot tensile properties, high retention of hardness, good toughness and resistance to heat checking, admits water cooling. BOHLER W303 is also ava.. |
|||
Tensile Strength, Yield | 1000 - 1380 MPa @Temperature 20.0 °C |
145000 - 200000 psi @Temperature 68.0 °F |
varies with heat treatment |
Bohler-Uddeholm BÖHLER W302 ISOBLOC® H13 hot work tool steel Properties:Hot work tool steel featuring excellent hot tensile properties, high hot wear resistance, adequate toughness and heat checking resistance, adequate toughness and heat checking; admits wat.. |