Mechanical Properties Metric English Comments
Tensile Strength, Yield 900 - 1100 MPa

@Strain 0.2 %
131000 - 160000 psi

@Strain 0.2 %
as built
EOS MS1 Maraging Steel for DMLS 3D Printing
EOS Maraging Steel MS1 is a steel powder which has been optimized especially for processing on EOSINT M 270 systems. This steel has very good mechanical properties, and is easily heat-treatable us..
Tensile Strength, Yield 1000 - 1100 MPa

@Strain 0.2 %
145000 - 160000 psi

@Strain 0.2 %
as built, XY direction
EOS PH1 Precipitation Hardening Stainless Steel for DMLS 3D Printing
EOS Stainless Steel PH1 is a stainless steel powder which has been optimized especially for processing on EOSINT M 270 systems. This stainless steel prototyping material is tough and resistant to ..