Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Tensile Strength, Yield | 110 MPa @Strain 0.200 %, Temperature 500 °C |
16000 psi @Strain 0.200 %, Temperature 932 °F |
EN min.; EN 10002-5 |
Outokumpu 4404 Cr-Ni-Mo Austenitic Stainless Steel General purpose steel with excellent corrosion resistance, particularly in the presence of halides.Applications: FiltersBraiding for hydraulic hosesShaftsFastenersMarine componentsAvailable in hot r.. |
|||
Tensile Strength, Yield | >= 110 MPa @Strain 0.200 % |
>= 16000 psi @Strain 0.200 % |
|
PSM Industries PolyAlloys MIM-2200 sintered Low Alloy Steel PolyAlloys Injected Metals, a division of PSM Industries, Inc., offers precision, High-Performance components for structural, magnetic and electronic applications that require a high degree of compl.. |
|||
Tensile Strength, Yield | >= 110 MPa @Temperature 250 °C |
>= 16000 psi @Temperature 482 °F |
|
PEAK Werkstoff DISPAL S542 Aluminum Alloy, AlMg6Mn4SiTiZrCo, Condition F Information provided by PEAK Werkstoff GmbH |
|||
Tensile Strength, Yield | 110 MPa @Temperature -40.0 °C |
16000 psi @Temperature -40.0 °F |
50%RH; ASTM D638 |
DuPont Performance Polymers Zytel® 101 NC010 Nylon 66
(Unverified Data**) Zytel® 101 NC010 is a general purpose polyamide 66 resin for injection molding and extrusion.Information provided by DuPont Performance Polymers |
|||
Tensile Strength, Yield | 110 MPa @Thickness 1.57 mm |
16000 psi @Thickness 0.0620 in |
CW; ASTM D638 |
Industrial Laminates/Norplex NP842 Paper Base Laminate
(discontinued **) Description: Paper reinforced phenolic grade with controlled conductivity. Mechanical strength similar to NP611. NP842 is semi-conductive on the surfaces and through the laminate.Thickness Tested: 0.. |
|||
Tensile Strength, Yield | 110 MPa @Thickness 1.57 mm |
16000 psi @Thickness 0.0620 in |
LW; ASTM D638 |
Industrial Laminates/Norplex NP329 Cotton Fabric Description: Bleached linen with melamine resin system. Provides better arc resistance than NP320E. Also, resistant to ammonia based refrigerants. Hard, durable material should be heated to punch, .. |
|||
Tensile Strength, Yield | 110 MPa @Thickness 1.57 mm |
16000 psi @Thickness 0.0620 in |
CW; ASTM D638 |
Industrial Laminates/Norplex NP660 Paper Base Laminate Description: Lower cost paper phenolic NEMA Grade XP. Uses natural kraft paper without pigmented cover sheet. Warm to hot punching. UL listed. Thickness Tested: 0.062", 0.125" & 0.500" |
|||
Tensile Strength, Yield | 110 MPa @Thickness 1.10 - 1.60 mm, Temperature 982 °C |
16000 psi @Thickness 0.0433 - 0.0630 in, Temperature 1800 °F |
0.2% offset |
Haynes Hastelloy® S alloy, flat products Nickel-based, high temperature alloy. Excellent thermal stability, low thermal expansion, excellent oxidation resistance to 1093°C, good high temperature and thermal fatigue strength. Application.. |
|||
Tensile Strength, Yield | >= 110 MPa @Strain 0.200 %, Thickness 150 - 500 mm |
>= 16000 psi @Strain 0.200 %, Thickness 5.91 - 19.7 in |
Temper 03 |
Constellium Alumold® 110 Aluminum Cast Sliced Plate Alumold®-110 has been specifically developed for low–pressure processing (thermoforming, RTM) of plastics and their composites. The material can also be used for prototype injection moulds. The ma.. |
|||
Tensile Strength, Yield | >= 110 MPa @Strain 0.200 %, Thickness 500 - 600 mm |
>= 16000 psi @Strain 0.200 %, Thickness 19.7 - 23.6 in |
Temper 03 |
Constellium Alumold® 110 Aluminum Cast Sliced Plate Alumold®-110 has been specifically developed for low–pressure processing (thermoforming, RTM) of plastics and their composites. The material can also be used for prototype injection moulds. The ma.. |
|||
Tensile Strength, Yield | >= 110 MPa @Strain 0.200 %, Thickness 150 - 500 mm |
>= 16000 psi @Strain 0.200 %, Thickness 5.91 - 19.7 in |
Temper O3 |
Constellium Fibral® Cast Aluminum Sliced Plate Fibral® has been specifically developed for low–pressure processing (thermoforming, RTM) of plastics and their composites. The material can also be used for prototype injection moulds. The materia.. |
|||
Tensile Strength, Yield | >= 110 MPa @Strain 0.200 %, Thickness 80.0 - 120 mm |
>= 16000 psi @Strain 0.200 %, Thickness 3.15 - 4.72 in |
Temper H111; Standard EN 485-2 |
Constellium PLAN 5083 Aluminum Rolled Plate Rolled plates in 5083 PLAN are optimized for minimum residual stress and improved dimensional tolerances. 5083 PLAN is mainly used for low stressed mechanical components, manufactured by intensive m.. |
|||
Tensile Strength, Yield | >= 110 MPa @Strain 0.200 %, Thickness 80.0 - 100 mm |
>= 16000 psi @Strain 0.200 %, Thickness 3.15 - 3.94 in |
Tempers O/H111; Standard EN 485-2 |
Constellium Planoxal® 50 Aluminum plate Planoxal®-50 plates differ from other standard EN-AW 5083 alloy products by their low level of residual stress. This specialty plate is also suitable for decorative anodizing. Planoxal®-50 is main.. |
|||
Tensile Strength, Yield | >= 110 MPa @Strain 0.200 %, Thickness 80.0 - 120 mm |
>= 16000 psi @Strain 0.200 %, Thickness 3.15 - 4.72 in |
Temper H111; Standard EN 485-2 |
Constellium ALPLAN® 5083 Rolled Precision Aluminum Plate, Milled Both Sides ALPLAN® 5083 precision plates exhibit good dimensional stability. Their low internal stresses reduces the effects of plate deformation during machining, thus saving on extra operations such as roug.. |