Braskem GD5160 HDPE Blow Molding Polyethylene Homopolymer

Category Polymer , Thermoplastic , Polyethylene (PE) , HDPE , High Density Polyethylene (HDPE), Blow Molding Grade
Manufacturer Braskem
Trade Name
Port Shanghai port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF Braskem GD5160 HDPE Blow Molding Polyethylene Homopolymer.pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
GD5160 is a high-density polyethylene homopolymer with high density and stiffness combined with high impact resistance and productivity. It was developed for the blow-molding segment. It is used in containers for yot, water, alcohol, cosmetics, lubricant oils, and water reservoirs.
Physical Properties Metric English Comments
Density 0.961 g/cc
0.0347 lb/in³
ASTM-D792
ESCR 100% Igepal® 20 hour

@Thickness 2.00 mm,
Temperature 50.0 °C
20 hour

@Thickness 0.0787 in,
Temperature 122 °F
0.3 mm notched-plaques; ASTM-D1693
ESCR 10% Igepal® 16 hour

@Thickness 2.00 mm,
Temperature 50.0 °C
16 hour

@Thickness 0.0787 in,
Temperature 122 °F
0.3 mm notched-plaques; ASTM-D1693
Melt Flow 0.65 g/10 min

@Load 2.16 kg,
Temperature 190 °C
0.65 g/10 min

@Load 4.76 lb,
Temperature 374 °F
ASTM-D1238
40 g/10 min

@Load 21.6 kg,
Temperature 190 °C
40 g/10 min

@Load 47.6 lb,
Temperature 374 °F
ASTM-D1238
Mechanical Properties Metric English Comments
Hardness, Shore D 63
63
ASTM-D2240
Tensile Strength at Break 36.0 MPa
5220 psi
ASTM-D638
Tensile Strength, Yield 30.0 MPa
4350 psi
ASTM-D638
Flexural Modulus, 1% Secant 1260 MPa
183000 psi
ASTM-D790
Izod Impact, Notched 1.20 J/cm
2.25 ft-lb/in
ASTM-D256
Thermal Properties Metric English Comments
Deflection Temperature at 0.46 MPa (66 psi) 79.0 °C
174 °F
ASTM-D648
Vicat Softening Point 128 °C

@Load 1.02 kg
262 °F

@Load 2.25 lb
ASTM-D1525