Polymer Property : Tensile Strength at Break = 21000 psi Product List

Mechanical Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Mechanical Properties Metric English Comments
Tensile Strength at Break 145 MPa

@Temperature 180 °C
21000 psi

@Temperature 356 °F
ISO 527
Victrex® PEEK 90HMF40 Polyetheretherketone (PEEK), 40% Carbon Fiber Reinforced
Product Description: High performance thermoplastic material, 40% carbon fiber reinforced PolyEtherEtherKetone (PEEK), semi crystalline, granules for injection molding, easy flow, color black.Typica..
Tensile Strength at Break 145 MPa

@Temperature 23.0 °C
21000 psi

@Temperature 73.4 °F
DAM; ISO 527
DuPont Performance Polymers Zytel® FE270038 BK267 Nylon 66  (Unverified Data**)
Zytel® FE270038 is a 40% glass fiber/mineral reinforced, heat stabilized polyamid 66 for injection molding. It is well suited for water injection technology.Information provided by DuPont Performan..
Tensile Strength at Break 145 MPa

@Temperature 23.0 °C
21000 psi

@Temperature 73.4 °F
50%RH; ISO 527
DuPont Performance Polymers Zytel® 73G45 BK263 Nylon 6  (Unverified Data**)
Zytel® 73G45 BK263 is a 45% glass fiber reinforced, black polyamide 6 resin for injection molding.Information provided by DuPont Performance Polymers
Tensile Strength at Break 145 MPa

@Temperature -10.0 °C
21000 psi

@Temperature 14.0 °F
ASTM D638
Gharda Chemicals G-PAEKâ„¢ 1230FC Ultra High Performance PEK Polymer
Product Details: Ultra High Performance Thermoplastic material, 10% carbon fiber, 10% PTFE and 10% graphite reinforced in Poly Aryl Ether Ketone, semi-crystalline granules suitable for injection mo..
Tensile Strength at Break 145 MPa

@Temperature 60.0 °C
21000 psi

@Temperature 140 °F
LATI Larpeek 10 GCE/600 PEEK, Glass/Mineral Reinforced
Polyetheretherketone (PEEK) based compound. Glass fibers / Mineral filler. Very good chemical resistance. Very good thermal properties. Low smoke density and low toxicity index.Availability: Africa ..
Tensile Strength at Break 145 MPa

@Temperature 60.0 °C
21000 psi

@Temperature 140 °F
LATI Larton GCE/600 PPS, Glass/Mineral Reinforced
Polyphenylene Sulfide (PPS) based compound. Glass fibers / Mineral filler. Very good chemical resistance. Very good thermal properties. Low smoke density and low toxicity index.Availability: Africa ..
Tensile Strength at Break 145 MPa

@Temperature 60.0 °C
21000 psi

@Temperature 140 °F
LATI Larton GCE/650 PPS, Glass/Mineral Reinforced
Polyphenylene Sulfide (PPS) based compound. Glass fibers / Mineral filler. Very good chemical resistance. Very good thermal properties. Low smoke density and low toxicity index.Availability: Africa ..
Tensile Strength at Break 145 MPa

@Temperature 90.0 °C
21000 psi

@Temperature 194 °F
LATI Larton K/40 HM PPS, 40% Carbon Fiber Reinforced
Polyphenylene Sulfide (PPS) based compound. Carbon fiber. High tensile modulus. Very good chemical resistance. Very good thermal properties. Low smoke density and low toxicity index.Availability: Af..
Tensile Strength at Break 145 MPa

@Temperature 23.0 °C
21000 psi

@Temperature 73.4 °F
LATI Latamid 6 H2 G/30-V0HF1 PA 6, 30% Glass Fiber Reinforced, Heat Stabilized, Flame Retardant
Polyamide 6 (PA6) based compound. Heat stabilized. Glass fibers. UL94 V-0 classified, halogens-based flame retardants and red phosphorous free. Very good electrical properties.Availability: Africa &..
Tensile Strength at Break 145 MPa

@Temperature 60.0 °C
21000 psi

@Temperature 140 °F
LATI Latamid 66 H2 G/35-V0KB PA 66, 35% Glass Fiber Reinforced, Heat Stabilized, Flame Retardant
Polyamide 66 (PA66) based compound. Heat stabilized. Glass fibers. UL94 V-0 classified, with red phosphorous. Availability: Africa & Middle East; Asia Pacific; Europe; Latin America; North AmericaIn..
Tensile Strength at Break 145 MPa

@Temperature 23.0 °C
21000 psi

@Temperature 73.4 °F
LATI Latamid 66 H2 G/35-V0KB3 PA 66, 35% Glass Fiber Reinforced, Heat Stabilized, Flame Retardant
Polyamide 66 (PA66) based compound. Heat stabilized. Glass fibers. UL94 V-0 classified, with red phosphorous. Availability: Africa & Middle East; Asia Pacific; Europe; Latin America; North AmericaIn..
Tensile Strength at Break 145 MPa

@Temperature 90.0 °C
21000 psi

@Temperature 194 °F
LATI Latamid 66 H2 K/40 PA 66, 40% Carbon Fiber Reinforced, Heat Stabilized
Polyamide 66 (PA66) based compound. Heat stabilized. Carbon fiber.Availability: Africa & Middle East; Asia Pacific; Europe; Latin America; North AmericaInformation provided by Lati Industria Termopl..
Tensile Strength at Break 145 MPa

@Temperature 23.0 °C
21000 psi

@Temperature 73.4 °F
LATI Larton L K/20 L-PPS, 20% Carbon Fiber Reinforced
Linear Polyphenylene Sulfide (L-PPS) based compound. Carbon fiber. Very good chemical resistance. Very good thermal properties. Low smoke density and low toxicity index.Availability: Africa & Middle..
Tensile Strength at Break 145 MPa

@Temperature 60.0 °C
21000 psi

@Temperature 140 °F
LATI Latamid 6 H2 G/65 PA 6, 65% Glass Fiber Reinforced, Heat Stabilized
Polyamide 6 (PA6) based compound. Heat stabilized. Glass fibers. Availability: Africa & Middle East; Asia Pacific; Europe; Latin America; North AmericaInformation provided by Lati Industria Termopla..
Tensile Strength at Break 145 MPa

@Temperature 23.0 °C
21000 psi

@Temperature 73.4 °F
LATI Latamid 66 H2 G/25-V0KB PA 66, 25% Glass Fiber Reinforced, Heat Stabilized, Flame Retardant
Polyamide 66 (PA66) based compound. Heat stabilized. Glass fibers. UL94 V-0 classified, with red phosphorous. Availability: Africa & Middle East; Asia Pacific; Europe; Latin America; North AmericaIn..
Tensile Strength at Break 145 MPa

@Temperature 23.0 °C
21000 psi

@Temperature 73.4 °F
LATI Latamid 66 H2 G/25-V0KB1 PA 66, 25% Glass Fiber Reinforced, Heat Stabilized, Flame Retardant
Polyamide 66 (PA66) based compound. Heat stabilized. Glass fibers. UL94 V-0 classified, with red phosphorous. Availability: Africa & Middle East; Asia Pacific; Europe; Latin America; North AmericaIn..
Tensile Strength at Break 145 MPa

@Temperature 23.0 °C
21000 psi

@Temperature 73.4 °F
LATI Latamid 66 VH G/30 PA 66, 30% Glass Fiber Reinforced, Heat Stabilized
Polyamide 66 (PA66) based compound. Heat stabilized. Hydrolysis stabilized. Glycol stabilized. Glass fibers.Availability: Africa & Middle East; Asia Pacific; Europe; Latin America; North AmericaInfo..
Tensile Strength at Break 145 MPa

@Temperature 23.0 °C
21000 psi

@Temperature 73.4 °F
LATI Latamid SP2 H2 G/35 PA 6.12, 35% Glass Fiber Reinforced, Heat Stabilized
Polyamide 6.12 (PA6.12) based compound. Heat stabilized. Glass fibers. Low moisture absorption.Availability: Africa & Middle East; Asia Pacific; Europe; Latin America; North AmericaInformation provi..
Tensile Strength at Break 145 MPa

@Temperature 23.0 °C
21000 psi

@Temperature 73.4 °F
LATI Laticonther 80 GCE/650 PPS, Glass/Mineral Reinforced
High thermal conductivity product based on Polyphenylene Sulfide (PPS). Glass fibers / Mineral filler.Availability: Africa & Middle East; Asia Pacific; Europe; Latin America; North AmericaInformatio..
Tensile Strength at Break 145 MPa

@Temperature 23.0 °C
21000 psi

@Temperature 73.4 °F
DAM; ISO 527
DuPont Performance Polymers Zytel® HTN FR52G30NHF BK337 Polyphthalamide (PPA)  (Unverified Data**)
Zytel® HTNFR52G30NHF BK337 is a 30% glass reinforced, flame retardant, lubricated high performance polyamide resin with improved flow. It is also a PPA resin and it uses a non-halogenated flame ret..
Tensile Strength at Break 145 MPa

@Temperature 60.0 °C
21000 psi

@Temperature 140 °F
LATI Latamid 66 H2 G/35 PA 66, 35% Glass Fiber Reinforced, Heat Stabilized
Polyamide 66 (PA66) based compound. Heat stabilized. Glass fibers. Availability: Africa & Middle East; Asia Pacific; Europe; Latin America; North AmericaInformation provided by Lati Industria Termop..
Tensile Strength at Break 145 MPa

@Temperature 23.0 °C
21000 psi

@Temperature 73.4 °F
ISO 527
BASF Ultramid® KR 4357 G6 30% Glass Filled PA6/6T (Conditioned)
Description: 30% glass-fiber reinforced, impact-modified product for injection-molding; high toughness, strength and stiffness, low water absorption, high melting point (295°C [563°F]). The mechan..