Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Tensile Strength at Break | 210 MPa @Temperature 23.0 °C |
30500 psi @Temperature 73.4 °F |
DAM; ISO 527 |
DuPont Performance Polymers Zytel® 70G35HSLRA4 BK267 Nylon 66
(Unverified Data**) Zytel® 70G35HSLRA4 BK267 is a 35% glass fiber reinforced, heat stabilized, hydrolysis resistant polyamide 66 resin for injection molding. It has excellent flow characteristics.Information provided .. |
|||
Tensile Strength at Break | 210 MPa @Temperature 23.0 °C |
30500 psi @Temperature 73.4 °F |
DAM; ISO 527 |
DuPont Performance Polymers Zytel® LM70G35HSLX BK314 Nylon 66
(Unverified Data**) Zytel® LM70G35HSLX is a 35% glass fiber reinforced, heat stabilized, lubricated polyamide 66 for injection molding. It is well suited for laser marking.Information provided by DuPont Performance Po.. |
|||
Tensile Strength at Break | 210 MPa @Temperature 60.0 °C |
30500 psi @Temperature 140 °F |
|
LATI Larpeek 10 G/50 PEEK, 50% Glass Fiber Reinforced Polyetheretherketone (PEEK) based compound. Glass fibers. Very good chemical resistance. Very good thermal properties. Low smoke density and low toxicity index.Availability: Africa & Middle East; As.. |
|||
Tensile Strength at Break | 210 MPa @Temperature 23.0 °C |
30500 psi @Temperature 73.4 °F |
|
LATI Latamid 66 H2 K/50 PA 66, 50% Carbon Fiber Reinforced, Heat Stabilized Polyamide 66 (PA66) based compound. Heat stabilized. Carbon fiber.Availability: Africa & Middle East; Asia Pacific; Europe; Latin America; North AmericaInformation provided by Lati Industria Termopl.. |
|||
Tensile Strength at Break | 210 MPa @Temperature 23.0 °C |
30500 psi @Temperature 73.4 °F |
|
LATI Larpeek 10 K/20 PEEK, 20% Carbon Fiber Reinforced Polyetheretherketone (PEEK) based compound. Carbon fiber. Very good chemical resistance. Very good thermal properties. Low smoke density and low toxicity index.Availability: Africa & Middle East; As.. |
|||
Tensile Strength at Break | 210 MPa @Temperature 23.0 °C |
30500 psi @Temperature 73.4 °F |
|
LATI Larpeek 10 K/40 HM PEEK, 40% Carbon Fiber Reinforced Polyetheretherketone (PEEK) based compound. Carbon fiber. High tensile modulus. Very good chemical resistance. Very good thermal properties. Low smoke density and low toxicity index.Availability: Af.. |
|||
Tensile Strength at Break | 210 MPa @Temperature 23.0 °C |
30500 psi @Temperature 73.4 °F |
|
LATI Latigloss 57 G/40 F2 PPA, 40% Glass Fiber Reinforced Product with high mechanical properties and exceptional surface finish based on Semi-aromatic polyamide (PPA). Glass fibers. Potentially suitable for food/medical contact applicationAvailability: Af.. |
|||
Tensile Strength at Break | 210 MPa @Temperature 90.0 °C |
30500 psi @Temperature 194 °F |
|
LATI Latigloss 57 G/60 F2 PPA, 60% Glass Fiber Reinforced Product with high mechanical properties and exceptional surface finish based on Semi-aromatic polyamide (PPA). Glass fibers. Potentially suitable for food/medical contact application. Availability: .. |
|||
Tensile Strength at Break | 210 MPa @Temperature 23.0 °C |
30500 psi @Temperature 73.4 °F |
DAM; ISO 527 |
DuPont Performance Polymers Zytel® PLUS PLS95G35DH1 BK031 Nylon Zytel® PLS95G35DH1 BK031is a high flow 35% glass reinforced PA using SHIELD Technology, only from DuPont, combining excellent surface appearance, excellent welding and fatigue retention, exceptiona.. |
|||
Tensile Strength at Break | 210 MPa @Temperature 180 °C |
30500 psi @Temperature 356 °F |
Dry; EN2561 |
Hexcel® HexTOOL™ M61 Quasi-isotropic High Temperature Prepreg Tooling Compound HexTOOL™ Tooling Compound is randomly layered strips of uni-directional prepreg which is consolidated into rolled goods. It can be utilized as multi-ply quasi-isotropic hand lay-up, and subsequentl.. |
|||
Tensile Strength at Break | 210 MPa @Temperature 23.0 °C |
30500 psi @Temperature 73.4 °F |
DAM; ISO 527 |
DuPont Performance Polymers Zytel® 70G35HSLX BK357 Nylon 66
(Unverified Data**) Zytel® 70G35HSLX BK357 is a 35% glass fiber reinforced, heat stabilized, black polyamide 66 for injection molding.Information provided by DuPont Performance Polymers |