Mechanical Properties Metric English Comments
Tensile Strength at Break >= 155 MPa

@Temperature 250 °C
>= 22500 psi

@Temperature 482 °F
PEAK Werkstoff DISPAL S542 Aluminum Alloy, AlMg6Mn4SiTiZrCo, Condition F
Information provided by PEAK Werkstoff GmbH
Tensile Strength at Break 155 MPa

@Temperature 90.0 °C
22500 psi

@Temperature 194 °F
LATI Laramid G/35 PPA, 35% Glass Fiber Reinforced
Semi-aromatic polyamide (PPA) based compound. Glass fibers. Very good thermal properties. Good chemical resistance. Low moisture absorption.Availability: Africa & Middle East; Asia Pacific; Europe; ..
Tensile Strength at Break 155 MPa

@Temperature 120 °C
22500 psi

@Temperature 248 °F
LATI Laramid G/50 PPA, 50% Glass Fiber Reinforced
Semi-aromatic polyamide (PPA) based compound. Glass fibers. Very good thermal properties. Good chemical resistance. Low moisture absorption.Availability: Africa & Middle East; Asia Pacific; Europe; ..
Tensile Strength at Break 155 MPa

@Temperature 90.0 °C
22500 psi

@Temperature 194 °F
LATI Larpeek 50 G/30 PEEK, 30% Glass Fiber Reinforced
Polyetheretherketone (PEEK) based compound. Glass fibers. Very good chemical resistance. Very good thermal properties. Low smoke density and low toxicity index.Availability: Africa & Middle East; As..
Tensile Strength at Break 155 MPa

@Temperature 120 °C
22500 psi

@Temperature 248 °F
LATI Larpeek 50 K/30 PEEK, 30% Carbon Fiber Reinforced
Polyetheretherketone (PEEK) based compound. Carbon fiber. Very good chemical resistance. Very good thermal properties. Low smoke density and low toxicity index.Availability: Africa & Middle East; As..
Tensile Strength at Break 155 MPa

@Temperature 90.0 °C
22500 psi

@Temperature 194 °F
LATI Larton GK/400 PPS, Glass/Carbon Fiber Reinforced
Polyphenylene Sulfide (PPS) based compound. Glass fibers / Carbon fibers. Very good chemical resistance. Very good thermal properties. Low smoke density and low toxicity index.Availability: Africa &..
Tensile Strength at Break 155 MPa

@Temperature 90.0 °C
22500 psi

@Temperature 194 °F
LATI Larpeek 10 G/30 PEEK, 30% Glass Fiber Reinforced
Polyetheretherketone (PEEK) based compound. Glass fibers. Very good chemical resistance. Very good thermal properties. Low smoke density and low toxicity index.Availability: Africa & Middle East; As..
Tensile Strength at Break 155 MPa

@Temperature 120 °C
22500 psi

@Temperature 248 °F
LATI Larpeek 10 K/40 HM PEEK, 40% Carbon Fiber Reinforced
Polyetheretherketone (PEEK) based compound. Carbon fiber. High tensile modulus. Very good chemical resistance. Very good thermal properties. Low smoke density and low toxicity index.Availability: Af..
Tensile Strength at Break 155 MPa

@Temperature 23.0 °C
22500 psi

@Temperature 73.4 °F
LATI Latamid 6 CUVHPX10 G/35 PA 6, 30% Glass Fiber Reinforced, Heat Stabilized
Polyamide 6 (PA6) based compound. High viscosity. Toughened. Glass fibers. Heat stabilized. UV stabilized. Good elongation.Availability: Africa & Middle East; Asia Pacific; Europe; Latin America; No..
Tensile Strength at Break 155 MPa

@Temperature 60.0 °C
22500 psi

@Temperature 140 °F
LATI Latamid SP1 G/50 PA 6.10, 50% Glass Fiber Reinforced
Polyamide 6.10 (PA6.10) based compound. Glass fibers. Low moisture absorption.Availability: Africa & Middle East; Asia Pacific; Europe; Latin America; North AmericaInformation provided by Lati Indus..
Tensile Strength at Break 155 MPa

@Temperature 60.0 °C
22500 psi

@Temperature 140 °F
LATI Latigloss 66 H2 K/30 PA 66, 30% Carbon Fiber Reinforced, Heat Stabilized
Product with high mechanical properties and exceptional surface finish based on Polyamide 66 (PA66). Heat stabilized. Carbon fiber. Availability: Africa & Middle East; Asia Pacific; Europe; Latin A..
Tensile Strength at Break 155 MPa

@Temperature 23.0 °C
22500 psi

@Temperature 73.4 °F
50%RH; ISO 527
DuPont Performance Polymers Zytel® HTN FR52G45BL BK337 Polyphthalamide (PPA)  (Unverified Data**)
Zytel® HTNFR52G45BL BK337 is a 45% glass reinforced, flame retardant, lubricated high performance polyamide resin that has been developed for connector applications.Information provided by DuPont ..