Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Izod Impact, Notched (ISO) | 5.40 kJ/m² @Temperature -30.0 °C |
2.57 ft-lb/in² @Temperature -22.0 °F |
ISO 180 |
Ascend Performance Materials Vydyne® R513H Black Nylon 66, 13% Glass Reinforced, Conditioned Vydyne® R513H Black is general-purpose, 13% glass-fiber reinforced, heat-stabilized PA66 resin. Available in black, it is an injection-molding grade that is lubricated for machine feed, flow, and m.. |
|||
Izod Impact, Notched (ISO) | 5.40 kJ/m² @Temperature -30.0 °C |
2.57 ft-lb/in² @Temperature -22.0 °F |
ISO 180 |
Ascend Performance Materials Vydyne® R513H Nylon 66, 13% Glass Filled, Conditioned (2.5% Moisture) Vydyne® R513H is general-purpose, 13% glass-reinforced, heat stabilized PA66 resin. Available in natural, it is an injection-molding grade resin that is lubricated for machine feed, flow, and mold .. |
|||
Izod Impact, Notched (ISO) | 5.40 kJ/m² @Temperature -30.0 °C |
2.57 ft-lb/in² @Temperature -22.0 °F |
ISO 180 |
Ascend Performance Materials Vydyne® R515 Nylon 66, 15% Glass Reinforced, Conditioned Vydyne® R515 is general-purpose, 15% glass-fiber reinforced PA66 resin. Availability:Asia PacificEuropeNorth AmericaFiller/Reinforcement:Glass Fiber, 15% Filler by WeightAdditive:Lubricant Features.. |
|||
Izod Impact, Notched (ISO) | 5.40 kJ/m² @Temperature -40.0 °C |
2.57 ft-lb/in² @Temperature -40.0 °F |
ISO 180 |
BASF Ultramid® TG3S 15% Glass Filled PA6 (Dry) Description: Ultramid TG3S is a 15% glass reinforced, heat stabilized, impact modified PA6 injection molding compound developed for applications requiring improved toughness in combination with a ba.. |
|||
Izod Impact, Notched (ISO) | 5.40 kJ/m² @Temperature 23.0 °C |
2.57 ft-lb/in² @Temperature 73.4 °F |
ISO 180 |
BASF Ultramid® B3GM35 BK 60564 40% Glass/Mineral Filled PA6 (Dry) Description: Ultramid B3GM35 BK60564 is a 40% combined glass-fiber and mineral reinforced, pigmented black injection molding PA6 grade.Applications: industrial articles requiring medium rigidity and.. |
|||
Izod Impact, Notched (ISO) | 5.40 kJ/m² @Temperature -30.0 °C |
2.57 ft-lb/in² @Temperature -22.0 °F |
ISO 180 |
Ascend Performance Materials Vydyne® R515H Nylon 66, 15% Glass Reinforced, Conditioned Vydyne® R515H is general-purpose, heat-stabilized, hydrolysis-resistant, 15% glass-fiber reinforced PA66 resin. Available in natural it is specifically designed to maximize the retention of physica.. |