Songhan Plastic Technology Co.,Ltd.
 POLYMER SEARCH

Eurotec® Tecodur® PB70 GR30 NL XA 21 PBT/PET 30% glass fiber reinforced, UL94 V0

Category Polymer , Thermoplastic , Polyester, TP , Polybutylene Terephthalate (PBT) , Polyethylene Terephthalate (PET)
Manufacturer Eurotec
Trade Name Tecodur®
Port Shanghai port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF Eurotec® Tecodur® PB70 GR30 NL XA 21 PBT/PET 30% glass fiber reinforced, UL94 V0.pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
Excellent stiffness and hardnessGood mechanical strengthGood creep and fatigue behaviorVery good thermal stabilityExcellent flammability characteristicsGood electrical propertiesHigh wear resistance and low frictionGood dimensional stabilityVery good chemical resistanceExcellent flow and processing propertiesLow moisture absorptionVery good surface finishAPPLICATIONS: AutomotiveElectrical/ElectronicBusiness equipmentConstructionHome appliances
Physical Properties Metric English Comments
Density 1.70 g/cc
0.0614 lb/in³
ISO 1183
Filler Content 30 %
30 %
ISO 3451
Moisture Absorption at Equilibrium 0.10 %
0.10 %
Humidity Absorption, 50% RH, 23°C; ISO 62
Water Absorption at Saturation 0.30 %
0.30 %
23°C; ISO 62
Linear Mold Shrinkage 0.0030 cm/cm
0.0030 in/in
Linear Mold Shrinkage, Transverse 0.010 cm/cm
0.010 in/in
Mechanical Properties Metric English Comments
Tensile Strength at Break 145 MPa
21000 psi
ISO 527
Elongation at Break 2.5 %
2.5 %
ISO 527
Tensile Modulus 11.5 GPa
1670 ksi
ISO 527
Izod Impact, Notched (ISO) 7.00 kJ/m²

@Temperature -30.0 °C
3.33 ft-lb/in²

@Temperature -22.0 °F
ISO 180/1A
8.00 kJ/m²

@Temperature 23.0 °C
3.81 ft-lb/in²

@Temperature 73.4 °F
ISO 180/1A
Charpy Impact Unnotched 4.00 J/cm²

@Temperature -30.0 °C
19.0 ft-lb/in²

@Temperature -22.0 °F
ISO 179/eU
4.50 J/cm²

@Temperature 23.0 °C
21.4 ft-lb/in²

@Temperature 73.4 °F
ISO 179/eU
Charpy Impact, Notched 0.800 J/cm²

@Temperature -30.0 °C
3.81 ft-lb/in²

@Temperature -22.0 °F
ISO 179/eA
0.900 J/cm²

@Temperature 23.0 °C
4.28 ft-lb/in²

@Temperature 73.4 °F
ISO 179/eA
Thermal Properties Metric English Comments
Melting Point 225 - 250 °C
437 - 482 °F
10 K/min; ISO 3146
Deflection Temperature at 0.46 MPa (66 psi) 220 °C
428 °F
ISO 75-1/2
Deflection Temperature at 1.8 MPa (264 psi) 210 °C
410 °F
ISO 75-1/2
Vicat Softening Point 210 °C
410 °F
50N; ISO 306
Flammability, UL94 V-0

@Thickness 1.60 mm
V-0

@Thickness 0.0630 in
V-0

@Thickness 3.20 mm
V-0

@Thickness 0.126 in
Glow Wire Test 960 °C

@Thickness 2.00 mm
1760 °F

@Thickness 0.0787 in
plaque; IEC 60695
Electrical Properties Metric English Comments
Volume Resistivity 1.00e+16 ohm-cm
1.00e+16 ohm-cm
IEC 60093
Surface Resistance 1.00e+14 ohm
1.00e+14 ohm
IEC 60093
Comparative Tracking Index 225 V
225 V
IEC 60112