Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Izod Impact, Notched (ISO) | 11.5 kJ/m² | 5.47 ft-lb/in² | ISO 180 |
Polycasa PETG QUINN PETG has good optical properties and a brilliant surface. The PETG range of sheets are easy to fabricate, to vacuum form, and show exceptional low temperature performance. Important benefits o.. |
|||
Izod Impact, Notched (ISO) | 11.5 kJ/m² @Temperature 23.0 °C |
5.47 ft-lb/in² @Temperature 73.4 °F |
ISO 180/A |
Victrex® PEEK 90GL60 Polyetheretherketone, 60% Glass Fibre Reinforced Product Description:High performance thermoplastic material, 60% glass fibre reinforced Polyetheretherketone (PEEK), semi crystalline, granules for injection moulding, standard flow, FDA food contac.. |
|||
Izod Impact, Notched (ISO) | 11.5 kJ/m² | 5.47 ft-lb/in² | ISO 180-1A |
Gromax BFG30-AS00N1 Nylon 6 30% Glass Filled (Dry) Information provided by Gromax Enterprises Corp. |
|||
Izod Impact, Notched (ISO) | 11.5 kJ/m² | 5.47 ft-lb/in² | GB/T 1843-2008 |
Sichuan Deyang Haton® hGR302 PPS / F4 Polyphenylene Sulfide Injection molding, anti-frictionInformation provided by Sichuan Deyang Chemical Co., LTD |
|||
Izod Impact, Notched (ISO) | 11.5 kJ/m² | 5.47 ft-lb/in² | ISO 180 |
Polyram PlusTek PA4501G6 Nylon 66, 30% Glass Fiber Reinforced, Low Friction 30% Glass fiber reinforced Nylon 66 for low friction applications.Information provided by Polyram. |
|||
Izod Impact, Notched (ISO) | 11.5 kJ/m² | 5.47 ft-lb/in² | ASTM D256 |
Total PSI 3341 High Impact Polystyrene Total Petrochemicals Polystyrene 3341 is a high impact polystyrene for the extrusion industry. Its good mechanical and thermal properties leads to the production of thermoformed articles of good ri.. |
|||
Izod Impact, Notched (ISO) | 11.5 kJ/m² @Temperature -40.0 °C |
5.47 ft-lb/in² @Temperature -40.0 °F |
ISO Test |
BASF Petra® 140 BK-112 45% Glass Filled PET Petra 140 BK-112 is a 45% glass reinforced, pigmented black, polyethylene terephthalate (PET) injection molding compound offering an increased level of strength, stiffness, high temperature performa.. |
|||
Izod Impact, Notched (ISO) | 11.5 kJ/m² | 5.47 ft-lb/in² | ISO 180/A |
BASF Ultramid® A3EG6 30% Glass Filled PA66 (Dry) Ultramid A3EG6 is a 30% glass fiber reinforced injection molding PA66 grade for machinery components and housings of high stiffness and dimensional stability. |
|||
Izod Impact, Notched (ISO) | 11.5 - 11.5 kJ/m² @Temperature -40.0 - -40.0 °C |
5.47 - 5.47 ft-lb/in² @Temperature -40.0 - -40.0 °F |
Average value: 11.5 kJ/m² Grade Count:1 |
Overview of materials for Polyethylene Terephthalate (PET), Glass Fiber Filled, Flame Retardant This property data is a summary of similar materials in the MatWeb database for the category "Polyethylene Terephthalate (PET), Glass Fiber Filled, Flame Retardant". Each property range of values re.. |