Polyram PlusTek PA4501G6 Nylon 66, 30% Glass Fiber Reinforced, Low Friction

Category Polymer , Thermoplastic , Nylon , Nylon 66 , Nylon 66, 30% Glass Fiber Filled
Manufacturer Polyram
Trade Name PlusTek
Port Shanghai port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF Polyram PlusTek PA4501G6 Nylon 66, 30% Glass Fiber Reinforced, Low Friction.pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
30% Glass fiber reinforced Nylon 66 for low friction applications.Information provided by Polyram.
Physical Properties Metric English Comments
Density 1.37 g/cc
0.0495 lb/in³
ISO 1183
Moisture Absorption at Equilibrium 1.7 %
1.7 %
50% RH; ISO 62
Linear Mold Shrinkage 0.0030 - 0.0040 cm/cm
0.0030 - 0.0040 in/in
ISO 2577
Mechanical Properties Metric English Comments
Hardness, Rockwell R 122
122
Tensile Strength, Yield 190 MPa
27600 psi
ISO 527
Elongation at Break 3.0 %
3.0 %
ISO 527
Flexural Strength 280 MPa
40600 psi
ISO 178
Flexural Modulus 8.80 GPa
1280 ksi
ISO 178
Izod Impact, Notched (ISO) 11.5 kJ/m²
5.47 ft-lb/in²
ISO 180
Thermal Properties Metric English Comments
Melting Point 256 °C
493 °F
ISO 11357
Maximum Service Temperature, Air 120 °C
248 °F
Continuous use
240 °C
464 °F
Short peaks operation
Deflection Temperature at 0.46 MPa (66 psi) 259 °C
498 °F
ISO 75
Deflection Temperature at 1.8 MPa (264 psi) 249 °C
480 °F
ISO 75
Flammability, UL94 HB

@Thickness 3.00 mm
HB

@Thickness 0.118 in
Electrical Properties Metric English Comments
Volume Resistivity 1.00e+15 ohm-cm
1.00e+15 ohm-cm
IEC 60093
Surface Resistance 1.00e+12 ohm
1.00e+12 ohm
IEC 60093
Dielectric Constant 3.5
3.5
IEC 60250
Dielectric Strength 90.0 kV/mm
2290 kV/in
IEC 60250
Users viewing this material also viewed the following: