Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Izod Impact, Notched (ISO) | 55.0 kJ/m² | 26.2 ft-lb/in² | 80*10*3; ISO 180/1A |
SABIC Innovative Plastics Cycoloy® RCY6113 PC+ABS (Asia Pacific) Cycoloy* RCY6113 resin is an injection moldable PC/ABS blend with non-brominated and non-chlorinated flame retardant. It contains 30% post consumer recycle content with a UL-94 5VB rating @ 2.0mm an.. |
|||
Izod Impact, Notched (ISO) | 55.0 kJ/m² | 26.2 ft-lb/in² | 80*10*4; ISO 180/1A |
SABIC Innovative Plastics Cycoloy® XCY620S PC+ABS (Europe-Africa-Middle East) PC+ ABS automotive applications, excellent flow/impact balance, high heat resistance temperature and excellent properties retention after hydrolytic and heat aging. |
|||
Izod Impact, Notched (ISO) | 55.0 kJ/m² | 26.2 ft-lb/in² | 80*10*3; ISO 180/1A |
SABIC Innovative Plastics Lexan® CFR9111 PC COPOLYMER (Asia Pacific) Lexan* CFR9111 Polycarbonate (PC) resin is a non-filled, injection moldable grade. This non-chlorinated, non-brominated flame retardant PC has an UL-94 V0 rating at 1.5 mm and good flow capability. .. |
|||
Izod Impact, Notched (ISO) | 55.0 kJ/m² | 26.2 ft-lb/in² | 80*10*3; ISO 180/1A |
SABIC Innovative Plastics Lexan® CFR9111 PC COPOLYMER (Europe-Africa-Middle East) Lexan* CFR9111 Polycarbonate (PC) resin is a non-filled, injection moldable grade. This non-chlorinated, non-brominated flame retardant PC has an UL-94 V0 rating at 1.5 mm and good flow capability. .. |
|||
Izod Impact, Notched (ISO) | 55.0 kJ/m² @Temperature -30.0 °C |
26.2 ft-lb/in² @Temperature -22.0 °F |
80*10*3; ISO 180/1A |
SABIC Innovative Plastics Lexan® EX1332T PC (Europe-Africa-Middle East) LEXAN* EX1332T polycarbonate resin, MVR (300C/1.2kg) 2 cm3/10min, high viscosity, branched, extrusion, mold release, UV stabilized, transparent, translucent and opaque colors. Multiwall sheet, Profi.. |
|||
Izod Impact, Notched (ISO) | 55.0 kJ/m² | 26.2 ft-lb/in² | 80*10*3; ISO 180/1A |
SABIC Innovative Plastics Lexan® EXL1112 PC Copolymer (Europe-Africa-Middle East) Lexan* EXL1112 polycarbonate (PC) siloxane copolymer resin is a high flow opaque injection molding (IM) grade. This resin offers good low temperature (-20 C) ductility in combination with excellent .. |
|||
Izod Impact, Notched (ISO) | 55.0 kJ/m² | 26.2 ft-lb/in² | 80*10*3; ISO 180/1A |
SABIC Innovative Plastics Lexan® EXL1132 PC Copolymer Lexan* EXL1132 polycarbonate (PC) siloxane copolymer resin is a high flow, UV stabilized injection molding grade. This resin offers good low temperature (-20 C) ductility in combination with high fl.. |
|||
Izod Impact, Notched (ISO) | 55.0 kJ/m² | 26.2 ft-lb/in² | 80*10*3; ISO 180/1A |
SABIC Innovative Plastics Lexan® EXL1132T PC Copolymer (Asia Pacific) Lexan* EXL1132T polycarbonate (PC) siloxane copolymer resin is a UV stabilized transparent injection molding (IM) grade with extra release properties. This resin offers good low temperature (-20 C) .. |
|||
Izod Impact, Notched (ISO) | 55.0 kJ/m² @Temperature -30.0 °C |
26.2 ft-lb/in² @Temperature -22.0 °F |
80*10*3; ISO 180/1A |
SABIC Innovative Plastics Lexan® EXL1330 PC Copolymer Lexan* EXL1330 polycarbonate (PC) siloxane copolymer resin is a UV stabilized opaque injection molding (IM) and sheet extrusion grade. This resin offers extreme low temperature (-60 C) ductility in .. |
|||
Izod Impact, Notched (ISO) | 55.0 kJ/m² @Temperature -30.0 °C |
26.2 ft-lb/in² @Temperature -22.0 °F |
80*10*3; ISO 180/1A |
SABIC Innovative Plastics Lexan® EXL1434T PC Copolymer (Europe-Africa-Middle East) Lexan* EXL1434T polycarbonate (PC) siloxane copolymer resin is a UV stabilized transparent injection molding grade. This resin offers extreme low temperature (-40 C) ductility in combination with me.. |
|||
Izod Impact, Notched (ISO) | 55.0 kJ/m² | 26.2 ft-lb/in² | 80*10*3; ISO 180/1A |
SABIC Innovative Plastics Lexan® EXL9112 PC Copolymer Opaque PC-Siloxane copolymer with excellent processability. Improved flow, low temp. ductility. Non-chlorinated, non-brominated flame retardant product. UL rated V-0/5VA. |
|||
Izod Impact, Notched (ISO) | 55.0 kJ/m² | 26.2 ft-lb/in² | 80*10*3; ISO 180/1A |
SABIC Innovative Plastics Lexan® HFD1930 PC Copolymer (Asia Pacific) 55 MFR LEXAN High Flow Ductile Copolymer, Natural color only |
|||
Izod Impact, Notched (ISO) | 55.0 kJ/m² @Temperature -30.0 °C |
26.2 ft-lb/in² @Temperature -22.0 °F |
80*10*3; ISO 180/1A |
SABIC Innovative Plastics Lexan® HPX4R PC Copolymer Medium flow specialty polycarbonate with outstanding processability, ductility and autoclavability. For medical devices and pharmaceutical applications. Healthcare management of change, biocompatib.. |
|||
Izod Impact, Notched (ISO) | 55.0 kJ/m² @Temperature -30.0 °C |
26.2 ft-lb/in² @Temperature -22.0 °F |
80*10*3; ISO 180/1A |
SABIC Innovative Plastics Lexan® HPX4R PC Copolymer (Asia Pacific) Medium flow specialty polycarbonate with outstanding processability, ductility and autoclavability. For medical devices and pharmaceutical applications. Healthcare management of change, biocompatib.. |
|||
Izod Impact, Notched (ISO) | 55.0 kJ/m² | 26.2 ft-lb/in² | 80*10*4; ISO 180/1A |
SABIC Innovative Plastics Lexan® ML6412 PC Copolymer ML6412 is an impact modified PC resin with non-brominated, non-chlorinated flame retardant system. |
|||
Izod Impact, Notched (ISO) | 55.0 kJ/m² @Temperature -30.0 °C |
26.2 ft-lb/in² @Temperature -22.0 °F |
80*10*3; ISO 180/1A |
SABIC Innovative Plastics Lexan® PK2870 PC LEXAN* PK2870 polycarbonate resin, global grade, MVR (300C/1.2kg) 2 cm3/10min, high viscosity, branched, blow molding, high melt strength, high impact resistance, Available in transparent colors onl.. |
|||
Izod Impact, Notched (ISO) | 55.0 kJ/m² @Temperature -30.0 °C |
26.2 ft-lb/in² @Temperature -22.0 °F |
80*10*3; ISO 180/1A |
SABIC Innovative Plastics Lexan® EX1632T PC (Europe-Africa-Middle East) LEXAN* EX1632T polycarbonate resin, MVR (300C/1.2kg) 6 cm3/10min, high viscosity, branched, extrusion, mold release, UV stabilized, transparent, translucent and opaque colors. Multiwall sheet, Profi.. |
|||
Izod Impact, Notched (ISO) | 55.0 kJ/m² @Temperature -30.0 °C |
26.2 ft-lb/in² @Temperature -22.0 °F |
80*10*3; ISO 180/1A |
SABIC Innovative Plastics Lexan® EXL1414T PC Copolymer (Asia Pacific) Lexan* EXL1414T polycarbonate (PC) siloxane copolymer resin is a transparent injection molding grade. This resin offers extreme low temperature (-40 °C) ductility in combination with medium flo.. |
|||
Izod Impact, Notched (ISO) | 55.0 kJ/m² | 26.2 ft-lb/in² | 80*10*3; ISO 180/1A |
SABIC Innovative Plastics Lexan® EXL9132 PC Copolymer (Asia Pacific) Opaque PC-Siloxane copolymer with excellent processability. Improved flow, low temperature ductility, UV stabilized. Non-chlorinated, non-brominated flame retardant product. UL rated V0/5VA. |
|||
Izod Impact, Notched (ISO) | 55.0 kJ/m² @Temperature -30.0 °C |
26.2 ft-lb/in² @Temperature -22.0 °F |
80*10*3; ISO 180/1A |
SABIC Innovative Plastics Lexan® EXL9330 PC Copolymer (Europe-Africa-Middle East) Opaque PC-Siloxane copolymer with excellent processability. Non-chlorinated, non-brominated flame retardant product in most colors. UV-stabilized. UL rated f1/V-0/5VA. |
|||
Izod Impact, Notched (ISO) | 55.0 kJ/m² | 26.2 ft-lb/in² | 80*10*3; ISO 180/1A |
SABIC Innovative Plastics Lexan® HFD1910 PC Copolymer 55 MFR LEXAN High Flow Ductile Copolymer, Natural colors only |
|||
Izod Impact, Notched (ISO) | 55.0 kJ/m² | 26.2 ft-lb/in² | 80*10*3; ISO 180/1A |
SABIC Innovative Plastics Lexan® HFD1910 PC Copolymer (Asia Pacific) 55 MFR LEXAN High Flow Ductile Copolymer, Natural colors only |
|||
Izod Impact, Notched (ISO) | 55.0 kJ/m² @Temperature 0.000 °C |
26.2 ft-lb/in² @Temperature 32.0 °F |
80*10*4; ISO 180/1A |
SABIC Innovative Plastics Xenoy® 5720U PBT+PC Unfilled PBT+PC alloy. Outstanding low temperature impact/chemical resistance. UV stabilized version of XENOY |
|||
Izod Impact, Notched (ISO) | 55.0 kJ/m² | 26.2 ft-lb/in² | 80*10*4; ISO 180/1A |
SABIC Innovative Plastics Xenoy® 5720U PBT+PC (Europe-Africa-Middle East) Unfilled PBT+PC alloy. Outstanding low temperature impact/chemical resistance. UV stabilized version of XENOY |
|||
Izod Impact, Notched (ISO) | 55.0 kJ/m² | 26.2 ft-lb/in² | 80*10*4; ISO 180/1A |
SABIC Innovative Plastics Xenoy® IQ1103R PBT+PC (Asia Pacific) Xenoy* Resin iQ1103R - Environmetally responsible, sustainable, and low carbon footprint resin. Xenoy iQ1103R is an unreinforced, impact modified PC + iQ-PBT alloy with excellent low temperature im.. |
|||
Izod Impact, Notched (ISO) | 55.0 kJ/m² | 26.2 ft-lb/in² | 80*10*4; ISO 180/1A |
SABIC Innovative Plastics Xenoy® IQ1103U PBT+PC Xenoy* Resin iQ1103U - Environmetally responsible, sustainable, and low carbon footprint resin. Xenoy iQ1103U is an unreinforced, UV stable, impact modified PC+ iQ-PBT alloy with excellent low temp.. |
|||
Izod Impact, Notched (ISO) | 55.0 kJ/m² | 26.2 ft-lb/in² | 80*10*4; ISO 180/1A |
SABIC Innovative Plastics Xenoy® IQ1103U PBT+PC (Europe-Africa-Middle East) Xenoy* Resin iQ1103U - Environmetally responsible, sustainable, and low carbon footprint resin. Xenoy iQ1103U is an unreinforced, UV stable, impact modified PC+ iQ-PBT alloy with excellent low temp.. |
|||
Izod Impact, Notched (ISO) | 55.0 kJ/m² @Temperature 23.0 °C |
26.2 ft-lb/in² @Temperature 73.4 °F |
80*10*4; ISO 180/1A |
SABIC Innovative Plastics LNP Thermotuf R1000IX4 PA 66 (Europe-Africa-Middle East) High Impact Nylon 66 compound containing Impact Modifier.This data was supplied by SABIC-IP for the Europe-Africa-Middle East region. |
|||
Izod Impact, Notched (ISO) | 55.0 kJ/m² | 26.2 ft-lb/in² | 80*10*4; ISO 180/1A |
SABIC Innovative Plastics Xenoy® XD1588 PBT+PC (Europe-Africa-Middle East) PBT+PC blend for painted automotive exterior applications, having good flow. |
|||
Izod Impact, Notched (ISO) | 55.0 kJ/m² | 26.2 ft-lb/in² | ISO 180/A |
Tisan TISSAN® Flame Retardant (V0) Styrene Acrylonitrile Properties:Natural or ColoredGlass fiber and glass beadMineral filledFlame retardantGood thermal and chemical resistanceExcellent transparencyExcellent mechanical propertiesDimensional stabilityEasy.. |