Songhan Plastic Technology Co.,Ltd.
 POLYMER SEARCH

Polymer Property : Izod Impact, Notched (ISO) = 55.0 kJ/m² Product List

Mechanical Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Mechanical Properties Metric English Comments
Izod Impact, Notched (ISO) 55.0 kJ/m²
26.2 ft-lb/in²
80*10*4; ISO 180/1A
SABIC Innovative Plastics Cycoloy® XCY620 PC+ABS (Asia Pacific)
PC+ ABS Automotive applications, High Impact and High Flow, ductility at low temperature, excellent properties retention after Hydrolytic and Heat Aging
Izod Impact, Notched (ISO) 55.0 kJ/m²
26.2 ft-lb/in²
80*10*4; ISO 180/1A
SABIC Innovative Plastics Cycoloy® XCY620HS PC+ABS
PC+ ABS General Purpose Non-FR
Izod Impact, Notched (ISO) 55.0 kJ/m²
26.2 ft-lb/in²
80*10*4; ISO 180/1A
SABIC Innovative Plastics Cycoloy® XCY620S PC+ABS (Europe-Africa-Middle East)
PC+ ABS automotive applications, excellent flow/impact balance, high heat resistance temperature and excellent properties retention after hydrolytic and heat aging.
Izod Impact, Notched (ISO) 55.0 kJ/m²
26.2 ft-lb/in²
80*10*3; ISO 180/1A
SABIC Innovative Plastics Lexan® CFR9111 PC COPOLYMER (Asia Pacific)
Lexan* CFR9111 Polycarbonate (PC) resin is a non-filled, injection moldable grade. This non-chlorinated, non-brominated flame retardant PC has an UL-94 V0 rating at 1.5 mm and good flow capability. ..
Izod Impact, Notched (ISO) 55.0 kJ/m²

@Temperature -30.0 °C
26.2 ft-lb/in²

@Temperature -22.0 °F
80*10*3; ISO 180/1A
SABIC Innovative Plastics Lexan® EX1332T PC (Europe-Africa-Middle East)
LEXAN* EX1332T polycarbonate resin, MVR (300C/1.2kg) 2 cm3/10min, high viscosity, branched, extrusion, mold release, UV stabilized, transparent, translucent and opaque colors. Multiwall sheet, Profi..
Izod Impact, Notched (ISO) 55.0 kJ/m²

@Temperature -30.0 °C
26.2 ft-lb/in²

@Temperature -22.0 °F
80*10*3; ISO 180/1A
SABIC Innovative Plastics Lexan® EXL1036 PC Copolymer (Asia Pacific)
Lexan* EXL1036 polycarbonate (PC) siloxane copolymer resin is a UV stabilized high viscosity grade designed for (co-)extrusion. This resin offers extreme low temperature (-60 C) ductility and good h..
Izod Impact, Notched (ISO) 55.0 kJ/m²
26.2 ft-lb/in²
80*10*3; ISO 180/1A
SABIC Innovative Plastics Lexan® EXL1112 PC Copolymer (Asia Pacific)
Lexan* EXL1112 polycarbonate (PC) siloxane copolymer resin is a high flow opaque injection molding (IM) grade. This resin offers good low temperature (-20 C) ductility in combination with excellent ..
Izod Impact, Notched (ISO) 55.0 kJ/m²

@Temperature -30.0 °C
26.2 ft-lb/in²

@Temperature -22.0 °F
80*10*3; ISO 180/1A
SABIC Innovative Plastics Lexan® EXL1413T PC Copolymer (Asia Pacific)
Lexan* EXL1413T polycarbonate (PC) siloxane copolymer resin is a transparent injection molding grade. This resin offers excellent low temperature (-30 °C) ductility in combination with medium f..
Izod Impact, Notched (ISO) 55.0 kJ/m²

@Temperature -30.0 °C
26.2 ft-lb/in²

@Temperature -22.0 °F
80*10*3; ISO 180/1A
SABIC Innovative Plastics Lexan® EXL1494T PC Copolymer
Lexan* EXL1494T polycarbonate (PC) siloxane copolymer resin is an injection molding grade with FDA and EU food contact compliance. This resin offers extreme low temperature (-40 C) ductility in comb..
Izod Impact, Notched (ISO) 55.0 kJ/m²
26.2 ft-lb/in²
80*10*3; ISO 180/1A
SABIC Innovative Plastics Lexan® EXL9112 PC Copolymer
Opaque PC-Siloxane copolymer with excellent processability. Improved flow, low temp. ductility. Non-chlorinated, non-brominated flame retardant product. UL rated V-0/5VA.
Izod Impact, Notched (ISO) 55.0 kJ/m²
26.2 ft-lb/in²
80*10*3; ISO 180/1A
SABIC Innovative Plastics Lexan® EXL9112 PC Copolymer (Asia Pacific)
Opaque PC-Siloxane copolymer with excellent processability. Improved flow, low temp. ductility. Non-chlorinated, non-brominated flame retardant product. UL rated V-0/5VA.
Izod Impact, Notched (ISO) 55.0 kJ/m²
26.2 ft-lb/in²
80*10*3; ISO 180/1A
SABIC Innovative Plastics Lexan® EXL9132 PC Copolymer
Opaque PC-Siloxane copolymer with excellent processability. Improved flow, low temperature ductility, UV stabilized. Non-chlorinated, non-brominated flame retardant product. UL rated V0/5VA.
Izod Impact, Notched (ISO) 55.0 kJ/m²

@Temperature -30.0 °C
26.2 ft-lb/in²

@Temperature -22.0 °F
80*10*3; ISO 180/1A
SABIC Innovative Plastics Lexan® FXE1112T PC Copolymer
Lexan* FXE1112T Lexan* polycarbonate (PC) siloxane copolymer resin is a transparent injection molding grade. This resin offers good low temperature (-20 C) ductility in combination with high flow ch..
Izod Impact, Notched (ISO) 55.0 kJ/m²

@Temperature -30.0 °C
26.2 ft-lb/in²

@Temperature -22.0 °F
80*10*3; ISO 180/1A
SABIC Innovative Plastics Lexan® HPX4R PC Copolymer (Asia Pacific)
Medium flow specialty polycarbonate with outstanding processability, ductility and autoclavability. For medical devices and pharmaceutical applications. Healthcare management of change, biocompatib..
Izod Impact, Notched (ISO) 55.0 kJ/m²
26.2 ft-lb/in²
80*10*4; ISO 180/1A
SABIC Innovative Plastics Lexan® ML6412 PC Copolymer
ML6412 is an impact modified PC resin with non-brominated, non-chlorinated flame retardant system.
Izod Impact, Notched (ISO) 55.0 kJ/m²

@Temperature -30.0 °C
26.2 ft-lb/in²

@Temperature -22.0 °F
80*10*3; ISO 180/1A
SABIC Innovative Plastics Lexan® PK2870 PC
LEXAN* PK2870 polycarbonate resin, global grade, MVR (300C/1.2kg) 2 cm3/10min, high viscosity, branched, blow molding, high melt strength, high impact resistance, Available in transparent colors onl..
Izod Impact, Notched (ISO) 55.0 kJ/m²

@Temperature -30.0 °C
26.2 ft-lb/in²

@Temperature -22.0 °F
80*10*3; ISO 180/1A
SABIC Innovative Plastics Lexan® EXL1414T PC Copolymer (Europe-Africa-Middle East)
Lexan* EXL1414T polycarbonate (PC) siloxane copolymer resin is a transparent injection molding grade. This resin offers extreme low temperature (-40 °C) ductility in combination with medium flo..
Izod Impact, Notched (ISO) 55.0 kJ/m²

@Temperature -30.0 °C
26.2 ft-lb/in²

@Temperature -22.0 °F
80*10*3; ISO 180/1A
SABIC Innovative Plastics Lexan® EXL9330 PC Copolymer (Asia Pacific)
Opaque PC-Siloxane copolymer with excellent processability. Non-chlorinated, non-brominated flame retardant product in most colors. UV-stabilized. UL rated f1/V-0/5VA.
Izod Impact, Notched (ISO) 55.0 kJ/m²

@Temperature -30.0 °C
26.2 ft-lb/in²

@Temperature -22.0 °F
80*10*3; ISO 180/1A
SABIC Innovative Plastics Lexan® FXD1413T PC Copolymer
Clear PC-siloxane copolymer with excellent processability, in special light diffusion colors. Medium flow. Improved toughness compared to medium flow standard PC in same color. Color package may af..
Izod Impact, Notched (ISO) 55.0 kJ/m²

@Temperature 0.000 °C
26.2 ft-lb/in²

@Temperature 32.0 °F
80*10*4; ISO 180/1A
SABIC Innovative Plastics Xenoy® 5720U PBT+PC (Europe-Africa-Middle East)
Unfilled PBT+PC alloy. Outstanding low temperature impact/chemical resistance. UV stabilized version of XENOY
Izod Impact, Notched (ISO) 55.0 kJ/m²
26.2 ft-lb/in²
80*10*4; ISO 180/1A
SABIC Innovative Plastics Xenoy® HX5600HP PBT+PC (Europe-Africa-Middle East)
Xenoy HX5600HP is PBT based semi-crystalline blend with balanced flow and impact properties. Improved chemical resistance against lab disinfectants and chemicals for healthcare enclosure and housing..
Izod Impact, Notched (ISO) 55.0 kJ/m²
26.2 ft-lb/in²
80*10*4; ISO 180/1A
SABIC Innovative Plastics Xenoy® IQ1103 PBT+PC
Xenoy iQ*1103 resin - Environmentally responsible and sustainable low carbon footprint resin. Xenoy iQ1103 is an unreinforced, impact modified alloy of PC (polycarbonate) + Valox iQ* PBT (polybuty..
Izod Impact, Notched (ISO) 55.0 kJ/m²
26.2 ft-lb/in²
80*10*4; ISO 180/1A
SABIC Innovative Plastics Xenoy® IQ1103 PBT+PC (Europe-Africa-Middle East)
Xenoy iQ*1103 resin - Environmentally responsible and sustainable low carbon footprint resin. Xenoy iQ1103 is an unreinforced, impact modified alloy of PC (polycarbonate) + Valox iQ* PBT (polybuty..
Izod Impact, Notched (ISO) 55.0 kJ/m²
26.2 ft-lb/in²
80*10*4; ISO 180/1A
SABIC Innovative Plastics Xenoy® IQ1103U PBT+PC (Europe-Africa-Middle East)
Xenoy* Resin iQ1103U - Environmetally responsible, sustainable, and low carbon footprint resin. Xenoy iQ1103U is an unreinforced, UV stable, impact modified PC+ iQ-PBT alloy with excellent low temp..
Izod Impact, Notched (ISO) 55.0 kJ/m²
26.2 ft-lb/in²
80*10*4; ISO 180/1A
SABIC Innovative Plastics Xenoy® X4820 PBT+PC (Asia Pacific)
Xenoy X4820 is a high modulus PC/PBT Blend. This resin provides high chemical resistance, excellent impact, very low creep, low CTE, excellent fatigue and dimensional stability.
Izod Impact, Notched (ISO) 55.0 kJ/m²
26.2 ft-lb/in²
80*10*4; ISO 180/1A
SABIC Innovative Plastics NORYL GTX GTX944 PPE+PA (Asia Pacific)
NORYL GTX944 is an unfilled GTX grade with improved processability and increased impact performance.
Izod Impact, Notched (ISO) 55.0 kJ/m²
26.2 ft-lb/in²
80*10*4; ISO 180/1A
SABIC Innovative Plastics NORYL GTX GTX944 PPE+PA (Europe-Africa-Middle East)
NORYL GTX944 is an unfilled GTX grade with improved processability and increased impact performance.
Izod Impact, Notched (ISO) 55.0 kJ/m²
26.2 ft-lb/in²
80*10*4; ISO 180/1A
SABIC Innovative Plastics Xenoy® XD1588 PBT+PC (Europe-Africa-Middle East)
PBT+PC blend for painted automotive exterior applications, having good flow.
Izod Impact, Notched (ISO) 55.0 kJ/m²
26.2 ft-lb/in²
80x10x4; ISO 180/1A
Eurostar Staramide R1000IX4 PA66, Impact Modified, Injection Molded
Staramide R1000IX4 is an Impact Modified Polyamide 66 Injection Molding Resin (also known as R1000HI020 Star X 1020)Information provided by Eurostar.
Izod Impact, Notched (ISO) 55.0 kJ/m²
26.2 ft-lb/in²
80*10*3; ISO 180/1A
SABIC Innovative Plastics Lexan® ML3485 PC (Europe-Africa-Middle East)
LEXAN ML3485 is a low viscosity grade exhibiting an improved ductility over standard polycarbonate grades at equal flow.
Copyright © lookpolymers.com All Rights Reserved