Dow LDPE 993I Low Density Polyethylene

Category Polymer , Thermoplastic , Polyethylene (PE) , LDPE , Low Density Polyethylene (LDPE), Molded
Manufacturer Dow Chemical
Trade Name
Port Shanghai port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF Dow LDPE 993I Low Density Polyethylene.pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
DOW LDPE 993I resin is a low slip, medium molecular weight distribution homopolymer designed to offer good gloss and rigidity with excellent flow characteristics. This resin has good processability over a wide range of molding conditions. This material complies with U.S.FDA regulation 21 CFR 177.1520(c) 2.1 for food contact applications. The regulation should be consulted for complete details.Data provided by Dow Chemical.
Physical Properties Metric English Comments
Density 0.925 g/cc
0.0334 lb/in³
Viscosity 28000 cP

@Shear Rate 5000 1/s,
Temperature 190 °C
28000 cP

@Shear Rate 5000 1/s,
Temperature 374 °F
Apparent Dynamic Viscosity
50000 cP

@Shear Rate 1000 1/s,
Temperature 190 °C
50000 cP

@Shear Rate 1000 1/s,
Temperature 374 °F
Apparent Dynamic Viscosity
76000 cP

@Shear Rate 300 1/s,
Temperature 190 °C
76000 cP

@Shear Rate 300 1/s,
Temperature 374 °F
Apparent Dynamic Viscosity
Melt Flow 25 g/10 min

@Load 2.16 kg
25 g/10 min

@Load 4.76 lb
Melt flow ratio I10/I2 is 9.1.
Mechanical Properties Metric English Comments
Tensile Strength, Ultimate 9.90 MPa
1440 psi
Tensile Strength, Yield 9.90 MPa
1440 psi
Elongation at Break 180 %
180 %
Modulus of Elasticity 0.186 GPa
27.0 ksi
Molded Sample 2% Secant Modulus
Flexural Modulus 0.291 GPa
42.2 ksi
Izod Impact, Notched (ISO) 32.0 kJ/m²

@Temperature -50.0 °C
15.2 ft-lb/in²

@Temperature -58.0 °F
Thermal Properties Metric English Comments
Vicat Softening Point 93.0 °C
199 °F