Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Izod Impact, Notched (ISO) | 1.90 - 1.90 kJ/m² @Temperature -40.0 - -40.0 °C |
0.904 - 0.904 ft-lb/in² @Temperature -40.0 - -40.0 °F |
Average value: 1.90 kJ/m² Grade Count:1 |
Overview of materials for Polypropylene with 40% Mica Filler This property data is a summary of similar materials in the MatWeb database for the category "Polypropylene with 40% Mica Filler". Specific grades with primary filler content between 35% and 44% are.. |