Polymer Property : Izod Impact, Unnotched (ISO) = 50.0 ft-lb/in² Product List

Mechanical Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Mechanical Properties Metric English Comments
Izod Impact, Unnotched (ISO) 55.0 - 105 kJ/m²
26.2 - 50.0 ft-lb/in²
Average value: 77.5 kJ/m² Grade Count:16
Overview of materials for Nylon 66, 40% Glass Fiber Filled
This property data is a summary of similar materials in the MatWeb database for the category "Nylon 66, 40% Glass Fiber Filled". Specific grades with glass content between 35% and 44% are included. ..
Izod Impact, Unnotched (ISO) 50.0 - 105 kJ/m²

@Temperature -40.0 - -30.0 °C
23.8 - 50.0 ft-lb/in²

@Temperature -40.0 - -22.0 °F
Average value: 73.8 kJ/m² Grade Count:9
Overview of materials for Nylon 66, 40% Glass Fiber Filled
This property data is a summary of similar materials in the MatWeb database for the category "Nylon 66, 40% Glass Fiber Filled". Specific grades with glass content between 35% and 44% are included. ..