Polymer Property : Charpy Impact Unnotched = 6.30 J/cm² Product List

Mechanical Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Mechanical Properties Metric English Comments
Charpy Impact Unnotched 6.30 J/cm²

@Temperature -20.0 °C
30.0 ft-lb/in²

@Temperature -4.00 °F
LATI Latamid 6 CUVHPX10 G/35 PA 6, 30% Glass Fiber Reinforced, Heat Stabilized
Polyamide 6 (PA6) based compound. High viscosity. Toughened. Glass fibers. Heat stabilized. UV stabilized. Good elongation.Availability: Africa & Middle East; Asia Pacific; Europe; Latin America; No..
Charpy Impact Unnotched 6.30 J/cm²

@Temperature 23.0 °C
30.0 ft-lb/in²

@Temperature 73.4 °F
ISO 179/1eU
Borealis Daplen™ EF341AE Polypropylene TPO Compound
Daplen™ EF341AE is a 30% mineral filled elastomer modified polypropylene compound intended for injection molding. This material has excellent balanced mechanical properties, gives a good surface q..
Charpy Impact Unnotched 6.30 J/cm²

@Temperature 23.0 °C
30.0 ft-lb/in²

@Temperature 73.4 °F
dry; ISO 179/1eU
DSM Novamid® 1010GN8-30 NAT PA6-GF30 FR
30% Glass Reinforced, Flame Retardant, Halogen free
Charpy Impact Unnotched 6.30 J/cm²

@Temperature -30.0 °C
30.0 ft-lb/in²

@Temperature -22.0 °F
ISO 179/1eU
Polyplastic Armamid® PA6 GF 30-2HSM-902 Nylon, 30% Glass Filled
Heat stabilizedInformation provided by PolyPlastic Group.