Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Charpy Impact Unnotched | 6.30 J/cm² @Temperature -20.0 °C |
30.0 ft-lb/in² @Temperature -4.00 °F |
|
LATI Latamid 6 CUVHPX10 G/35 PA 6, 30% Glass Fiber Reinforced, Heat Stabilized Polyamide 6 (PA6) based compound. High viscosity. Toughened. Glass fibers. Heat stabilized. UV stabilized. Good elongation.Availability: Africa & Middle East; Asia Pacific; Europe; Latin America; No.. |
|||
Charpy Impact Unnotched | 6.30 J/cm² @Temperature 23.0 °C |
30.0 ft-lb/in² @Temperature 73.4 °F |
ISO 179/1eU |
Borealis Daplen™ EF341AE Polypropylene TPO Compound Daplen™ EF341AE is a 30% mineral filled elastomer modified polypropylene compound intended for injection molding. This material has excellent balanced mechanical properties, gives a good surface q.. |
|||
Charpy Impact Unnotched | 6.30 J/cm² @Temperature 23.0 °C |
30.0 ft-lb/in² @Temperature 73.4 °F |
dry; ISO 179/1eU |
DSM Novamid® 1010GN8-30 NAT PA6-GF30 FR 30% Glass Reinforced, Flame Retardant, Halogen free |
|||
Charpy Impact Unnotched | 6.30 J/cm² @Temperature -30.0 °C |
30.0 ft-lb/in² @Temperature -22.0 °F |
ISO 179/1eU |
Polyplastic Armamid® PA6 GF 30-2HSM-902 Nylon, 30% Glass Filled Heat stabilizedInformation provided by PolyPlastic Group. |