Mechanical Properties Metric English Comments
Charpy Impact Unnotched 3.80 J/cm²

@Temperature -20.0 °C
18.1 ft-lb/in²

@Temperature -4.00 °F
STN EN ISO 179
Plastcom SLOVALEN PC 69 GF 35 FRT 4 Polypropylene Copolymer, 35% Glass Fiber, Halogen Free and Phosphor Free Flame Retardant
FeaturesModified copolymer PP for injection moulding, chemically reinforced with 35% glass fiber, contains the modifier of mechanical properties and non halogen and free phosphor flame retardant. I..
Charpy Impact Unnotched 3.80 J/cm²

@Temperature -20.0 °C
18.1 ft-lb/in²

@Temperature -4.00 °F
Plastcom SLOVAMID 6 GF 25 FRC 3 PA6, 25% glass fibre, flame retardant
FeaturesPA 6 for injection moulding, chemically strengthened with 25 % glass fibre. Application: impacted mouldings and mouldings with high strength applied in automotive, electrical, engineering an..
Charpy Impact Unnotched 3.80 J/cm²

@Temperature -20.0 °C
18.1 ft-lb/in²

@Temperature -4.00 °F
Plastcom SLOVAMID 6/66 GF 20 T 10 FRG 5 PA6/66, 20% glass fibre, flame retardant
Packaging, transport, stockingThe product is packed in hermetically closed thick-walled 25 kg PE bags, on a 1.000 kg palette coated in a stretch foil, in big bags with a thick PE foil fixed on a 1.0..
Charpy Impact Unnotched 3.80 J/cm²

@Temperature 23.0 °C
18.1 ft-lb/in²

@Temperature 73.4 °F
Edgew 80*10*3 sp=62mm; ISO 179/1eU
SABIC Innovative Plastics Cycoloy® C4215HF PC+ABS (Europe-Africa-Middle East)
Cycoloy C4215HF is a 15% glass reinforced, non-FR PC+ABS grade with high heat resistance, excellent strength and rigidity with good cosmetic apprearance. It combines good processability with a low s..
Charpy Impact Unnotched 3.80 J/cm²

@Temperature 23.0 °C
18.1 ft-lb/in²

@Temperature 73.4 °F
DAM; ISO 179/1eU
DuPont Performance Polymers Zytel® HTN FG52G35HSL BK011 Polyphthalamide (PPA)  (Unverified Data**)
Zytel®® HTNFG52G35HSL BK011 is a 35% glass reinforced, lubricated, heat stabilized high performance polyamide resin, developed for consideration into applications for the food industry. It is also..
Charpy Impact Unnotched 3.80 J/cm²

@Temperature 23.0 °C
18.1 ft-lb/in²

@Temperature 73.4 °F
50%RH; ISO 179/1eU
DuPont Performance Polymers Zytel® HTN FG52G35HSL BK011 Polyphthalamide (PPA)  (Unverified Data**)
Zytel®® HTNFG52G35HSL BK011 is a 35% glass reinforced, lubricated, heat stabilized high performance polyamide resin, developed for consideration into applications for the food industry. It is also..
Charpy Impact Unnotched 3.80 J/cm²

@Temperature -30.0 °C
18.1 ft-lb/in²

@Temperature -22.0 °F
Radici Radilon® S RCV3015 (cond.) Nylon 6
Radilon® S is a range of polyamide 6 (PA6) products obtained through the polymerization of caprolactam and used for injection, extrusion and blow-molding.Information provided by Radici group.
Charpy Impact Unnotched 3.80 J/cm²

@Temperature 23.0 °C
18.1 ft-lb/in²

@Temperature 73.4 °F
ISO 179/1eU
Lanxess Durethan® BM 25 FN20 700350 Nylon 6, 25% Mineral
PA 6, injection molding grade, 25% mineral, UL94V-2 off 0.75 mm, max. temp. glow wire test:960°C off 0.8 mm, free from halogen
Charpy Impact Unnotched 3.80 J/cm²

@Temperature -20.0 °C
18.1 ft-lb/in²

@Temperature -4.00 °F
LATI Latan 13 S/30 POM, 30% Glass Bead Reinforced
Polyoxymethylene (POM) based compound. Glass beads. Medium viscosity. High dimensional stability.Availability: Africa & Middle East; Asia Pacific; Europe; Latin America; North AmericaInformation pro..
Charpy Impact Unnotched 3.80 J/cm²

@Temperature -30.0 °C
18.1 ft-lb/in²

@Temperature -22.0 °F
ISO 179/1eU
Sax Polymers SAXAMID 126F3 Nylon 6, 15% Glass Fiber
SAXAMID 126F3 is a polyamide 6 injection-molding-grade reinforced with 15% glass fibers.Information provided by SAX Polymers
Charpy Impact Unnotched 3.80 J/cm²

@Temperature 23.0 °C
18.1 ft-lb/in²

@Temperature 73.4 °F
ISO 179/1eU
Borealis MS64T20 Polypropylene Compound, Mineral Filled
MS64T20 is a 20% mineral filled polypropylene compound intended for injection molding. This material has excellent balanced mechanical properties and is easy to process. Applications: automotive p..
Charpy Impact Unnotched 3.80 J/cm²

@Temperature 23.0 °C
18.1 ft-lb/in²

@Temperature 73.4 °F
dry; ISO 179/1eU
DSM Novamid® 1010GN2-20 NAT/BK37 PA6-GF20 FR(17)
20% Glass Reinforced, Flame Retardant
Charpy Impact Unnotched 3.80 J/cm²

@Temperature 23.0 °C
18.1 ft-lb/in²

@Temperature 73.4 °F
ISO 179
Ascend Performance Materials Vydyne® R513H Black Nylon 66, 13% Glass Reinforced, DAM
Vydyne® R513H Black is general-purpose, 13% glass-fiber reinforced, heat-stabilized PA66 resin. Available in black, it is an injection-molding grade that is lubricated for machine feed, flow, and m..
Charpy Impact Unnotched 3.80 J/cm²

@Temperature -30.0 °C
18.1 ft-lb/in²

@Temperature -22.0 °F
ISO 179
Ascend Performance Materials Vydyne® R515 Nylon 66, 15% Glass Reinforced, Conditioned
Vydyne® R515 is general-purpose, 15% glass-fiber reinforced PA66 resin. Availability:Asia PacificEuropeNorth AmericaFiller/Reinforcement:Glass Fiber, 15% Filler by WeightAdditive:Lubricant Features..
Charpy Impact Unnotched 3.80 J/cm²

@Temperature 23.0 °C
18.1 ft-lb/in²

@Temperature 73.4 °F
ISO 179/1eU
Akro-Plastic Akromid® A3 GF 10 (2852) PA 6.6 Dry, 10% Glass Filled
AKROMID® A (Polyamide 6.6) is an engineering compound, characterized by high mechanical strength, stiffness and thermal resistance. Furthermore, this polyamide offers high toughness at low temperat..
Charpy Impact Unnotched 3.80 J/cm²

@Temperature 23.0 °C
18.1 ft-lb/in²

@Temperature 73.4 °F
ISO 179
Ascend Performance Materials Vydyne® R513H Nylon 66, 13% Glass Filled, Dry as Molded
Vydyne® R513H is general-purpose, 13% glass-reinforced, heat stabilized PA66 resin. Available in natural, it is an injection-molding grade resin that is lubricated for machine feed, flow, and mold ..
Charpy Impact Unnotched 3.80 J/cm²

@Temperature -30.0 °C
18.1 ft-lb/in²

@Temperature -22.0 °F
ISO 179
Ascend Performance Materials Vydyne® R515H Nylon 66, 15% Glass Reinforced, Conditioned
Vydyne® R515H is general-purpose, heat-stabilized, hydrolysis-resistant, 15% glass-fiber reinforced PA66 resin. Available in natural it is specifically designed to maximize the retention of physica..
Charpy Impact Unnotched 3.80 J/cm²

@Temperature 23.0 °C
18.1 ft-lb/in²

@Temperature 73.4 °F
ISO 179/1eU
Lanxess Durethan® BM 25 FN20 DUS013 000000 Nylon 6, 25% Mineral
PA 6, injection molding grade, 25% mineral, UL94V-2 off 0.75 mm, max. temp. glow wire test:960°C off 0.8 mm, free from halogen, optimized for laser marking at 1064 nm,
Charpy Impact Unnotched 3.80 J/cm²

@Temperature -30.0 °C
18.1 ft-lb/in²

@Temperature -22.0 °F
ISO 179/1eU
BASF Ultradur® B 4300 G2 FC 10% Glass Filled PBT
Description: The BASF Ultradur® FC (Food Contact) grades enable the industry to develop products for food contact applications which are in compliance with multiple regional food contact regulation..