Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Tensile Strength at Break | >= 620 MPa | >= 89900 psi | 20.4 lb. Minimum Tensile Load 0.017 in. Diameter |
Shakespeare FL-8 Fluorocarbon PVDF Fishing Line, 17 lb 100% pure PVDF fluoro-polymer, great clarity, limpness and strength, low refractive index that decreases the visibility of the line.Information provided by Shakespeare Company. |
|||
Tensile Strength at Break | 620 - 880 MPa | 89900 - 128000 psi | |
Schmolz + Bickenbach UGICHROM 4460 Duplex Chrome Plated Bar Description: Ugichrom combines the high efficiency of micro-fissuring chromium plating with the technology of Ugitech’s most advanced gradesAdvantages: Zero defects guarantee; Low friction coef.. |
|||
Tensile Strength at Break | 620 - 780 MPa | 89900 - 113000 psi | |
Goodfellow T1-Thermocouple Alloy The positive element of the type K thermocouple alloy the negative being T2. The thermocouple can be used up to 1250C in oxidizing atmospheres and is the probably the most common in use. It is also .. |
|||
Tensile Strength at Break | 620 MPa | 89900 psi | |
ThyssenKrupp TBL PLUS Structural Steel This Material Specification applies to heavy plate with thicknesses up to 12 mm, made of the fine-grain structural steel TBL PLUS.Application: The steel may be used for welded constructions of diffe.. |