Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Tensile Strength at Break | 650 - 880 MPa | 94300 - 128000 psi | |
Schmolz + Bickenbach UGICHROM 4362 Chrome Plated Bar Description: Ugichrom combines the high efficiency of micro-fissuring chromium plating with the technology of Ugitech’s most advanced gradesAdvantages: Zero defects guarantee; Low friction coef.. |
|||
Tensile Strength at Break | 620 - 880 MPa | 89900 - 128000 psi | |
Schmolz + Bickenbach UGICHROM 4460 Duplex Chrome Plated Bar Description: Ugichrom combines the high efficiency of micro-fissuring chromium plating with the technology of Ugitech’s most advanced gradesAdvantages: Zero defects guarantee; Low friction coef.. |
|||
Tensile Strength at Break | 650 - 880 MPa | 94300 - 128000 psi | |
Schmolz + Bickenbach UGICHROM 4462 Duplex Chrome Plated Bar Description: Ugichrom combines the high efficiency of micro-fissuring chromium plating with the technology of Ugitech’s most advanced gradesAdvantages: Zero defects guarantee; Low friction coef.. |
|||
Tensile Strength at Break | 700 - 880 MPa | 102000 - 128000 psi | |
ThyssenKrupp PAS 650 Structural Steel for Cold Forming This Material Specification applies to plates made of low carbon high strength steels with minimum yield strength values between 315 and 700 MPa1) in the thermo mechanically rolled delivery conditio.. |