Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Tensile Strength at Break | 550 - 780 MPa | 79800 - 113000 psi | |
Goodfellow T2-Thermocouple Alloy The negative element of the type K thermocouple, the positive being T1. The thermocouple can be used up to 1250C in oxidizing atmospheres, and probably is the most common in use.Information provided.. |
|||
Tensile Strength at Break | 620 - 780 MPa | 89900 - 113000 psi | |
Goodfellow T1-Thermocouple Alloy The positive element of the type K thermocouple alloy the negative being T2. The thermocouple can be used up to 1250C in oxidizing atmospheres and is the probably the most common in use. It is also .. |