Polymer Property : Tensile Strength at Break = 8.10 MPa Product List

Mechanical Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Mechanical Properties Metric English Comments
Tensile Strength at Break 8.10 MPa
1170 psi
ASTM D412
Sumitomo Chemical ESPOLEX® 4855 Thermoplastic Elastomer
ESPOLEX® TPE Series is a group of thermoplastic elastomers produced by Sumitomo Chemical Company. Among its material advantages, ESPOLEX® TPE Series is distinguished by offering many low-densi..
Tensile Strength at Break 8.10 MPa
1170 psi
Across Flow; ASTM D412 and ISO 37
ExxonMobil Santoprene® 121-65B200 Thermoplastic Vulcanizate - UV Resistant
Product Description: A soft, black, UV resistant thermoplastic vulcanizate (TPV) in the thermoplastic elastomer (TPE) family. This material is specially formulated to bond to thermoset EPDM rubber ..
Tensile Strength at Break 8.10 MPa
1170 psi
Across Flow; ASTM D412 and ISO 37
ExxonMobil Santoprene® 191-85PA12 Thermoplastic Vulcanizate  (discontinued **)
Product Description: A black, specialty thermoplastic vulcanizate (TPV) in the thermoplastic elastomer (TPE) family. It is especially formulated to bond to PA-12 for applications such as co-extrude..