Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Tensile Strength at Break | 8.10 MPa | 1170 psi | ASTM D412 |
Sumitomo Chemical ESPOLEX® 4855 Thermoplastic Elastomer ESPOLEX® TPE Series is a group of thermoplastic elastomers produced by Sumitomo Chemical Company. Among its material advantages, ESPOLEX® TPE Series is distinguished by offering many low-densi.. |
|||
Tensile Strength at Break | 8.07 MPa | 1170 psi | ASTM D412 |
Teknor Apex Telcar® TL-91-T3056S-90 Thermoplastic Elastomer Uses: Automotive Applications; Automotive Exterior Parts; Automotive Exterior Trim; Automotive Interior Parts; Blow Molding Applications; General Purpose; Grommets; Weatherstripping Forms: Pellets .. |
|||
Tensile Strength at Break | 8.10 MPa | 1170 psi | Across Flow; ASTM D412 and ISO 37 |
ExxonMobil Santoprene® 121-65B200 Thermoplastic Vulcanizate - UV Resistant Product Description: A soft, black, UV resistant thermoplastic vulcanizate (TPV) in the thermoplastic elastomer (TPE) family. This material is specially formulated to bond to thermoset EPDM rubber .. |
|||
Tensile Strength at Break | 8.10 MPa | 1170 psi | Across Flow; ASTM D412 and ISO 37 |
ExxonMobil Santoprene® 191-85PA12 Thermoplastic Vulcanizate
(discontinued **) Product Description: A black, specialty thermoplastic vulcanizate (TPV) in the thermoplastic elastomer (TPE) family. It is especially formulated to bond to PA-12 for applications such as co-extrude.. |
|||
Tensile Strength at Break | 8.04 MPa @Temperature 25.0 °C, Time 259000 sec |
1170 psi @Temperature 77.0 °F, Time 72.0 hour |
Fluid Aging ASTM Fuel D |
LG Chemical NBR 8300 High Acrylonitrile Polymer Description: NBR 8300 is a copolymer of butadiene-acrylonitrile and the powdered nitrile elastomer manufactured by advanced emulsion polymerization technology of Goodyear and LG Chem. NBR 8300 has .. |