Songhan Plastic Technology Co.,Ltd.
 POLYMER SEARCH

ExxonMobil Santoprene® 121-65B200 Thermoplastic Vulcanizate - UV Resistant

Category Polymer , Thermoplastic , Elastomer, TPE , Thermoplastic Vulcanizate Elastomer (TPV)
Manufacturer Exxon Chemical
Trade Name Santoprene®
Port Shanghai port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF ExxonMobil Santoprene® 121-65B200 Thermoplastic Vulcanizate - UV Resistant.pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
Product Description: A soft, black, UV resistant thermoplastic vulcanizate (TPV) in the thermoplastic elastomer (TPE) family. This material is specially formulated to bond to thermoset EPDM rubber for corner molding, end caps and special applications requiring such adhesion to thermoset EPDM. This grade of Santoprene TPV is shear-dependent and can be processed on conventional thermoplastics equipment for injection molding. It is polyolefin based and completely recyclable.Key Features:Adheres to vulcanized EPDM rubber over wide range of temperatures.High flexibility targeted for dynamic EPDM applications.Higher gloss enables matching EPDM mating surface.Used in sealing applications.EU and China RoHS compliant.Processing Method: Injection Molding and Multi Injection MoldingAvailability: Africa & Middle East, Europe, North America, Asia Pacific, Latin America and South AmericaInformation provided by ExxonMobil Chemical.
Physical Properties Metric English Comments
Specific Gravity 0.910 g/cc
0.910 g/cc
ASTM D792 and ISO 1183
Mechanical Properties Metric English Comments
Hardness, Shore A 64
64
2 mm; ISO 868
Tensile Strength at Break 8.10 MPa
1170 psi
Across Flow; ASTM D412 and ISO 37
Tensile Stress 2.30 MPa

@Strain 100 %
334 psi

@Strain 100 %
Across Flow; ASTM D412 and ISO 37
Elongation at Break 600 %
600 %
Across Flow; ASTM D412 and ISO 37
Compression Set 22 %

@Temperature 23.0 °C,
Time 79200 sec
22 %

@Temperature 73.4 °F,
Time 22.0 hour
ASTM D395B Type 1 and ISO 188 Type A
48 %

@Temperature 70.0 °C,
Time 79200 sec
48 %

@Temperature 158 °F,
Time 22.0 hour
ASTM D395B Type 1 and ISO 188 Type A
53 %

@Temperature 70.0 °C,
Time 605000 sec
53 %

@Temperature 158 °F,
Time 168 hour
ASTM D395B Type 1 and ISO 188 Type A
Copyright © lookpolymers.com All Rights Reserved