Songhan Plastic Technology Co.,Ltd.
 POLYMER SEARCH

ExxonMobil Santoprene® 191-85PA12 Thermoplastic Vulcanizate  (discontinued **)

Category Polymer , Thermoplastic , Elastomer, TPE , Thermoplastic Vulcanizate Elastomer (TPV)
Manufacturer
Trade Name
Port Ningbo port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF ExxonMobil Santoprene® 191-85PA12 Thermoplastic Vulcanizate  (discontinued **).pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
Product Description: A black, specialty thermoplastic vulcanizate (TPV) in the thermoplastic elastomer (TPE) family. It is especially formulated to bond to PA-12 for applications such as co-extruded, thermoformed automotive coolant hose. This grade of Santoprene TPV is shear-dependent and can be processed on conventional thermoplastics equipment for injection molding or extrusion. It is polyolefin based and completely recyclable.Key Features:Designed for excellent adhesion to PA-12 even after thermoforming of co-extruded corrugated tubes.EU and China RoHS compliant.Information provided by ExxonMobil Chemical.
Physical Properties Metric English Comments
Specific Gravity 0.970 g/cc
0.970 g/cc
ASTM D792 and ISO 1183
Mechanical Properties Metric English Comments
Hardness, Shore A 87

@Time 15.0 sec
87

@Time 0.00417 hour
2 mm; ISO 868
Tensile Strength at Break 8.10 MPa
1170 psi
Across Flow; ASTM D412 and ISO 37
Tensile Stress 5.00 MPa

@Strain 100 %
725 psi

@Strain 100 %
Across Flow; ASTM D412 and ISO 37
Elongation at Break 350 %
350 %
Across Flow; ASTM D412 and ISO 37
Users viewing this material also viewed the following: