Polymer Property : Tensile Strength at Break = 39900 psi Product List

Mechanical Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Mechanical Properties Metric English Comments
Tensile Strength at Break 275 MPa
39900 psi
5 mm/min; ISO 527
SABIC Innovative Plastics LNP THERMOCOMP UX06003 PPA (Europe-Africa-Middle East)
LNP* THERMOCOMP* UX06003 is a compound based on Polyphalamide resin containing Carbon Fiber. Added features include Electrically Conductive, Mold Release, Heat Stabilized.
Tensile Strength at Break 275 MPa
39900 psi
ISO 527-2
Solvay Specialty Polymers Amodel® A-8950 HS Polyphthalamide (PPA), 50% Glass Fiber
Amodel® A-8950 HS is a 50% glass-fiber-reinforced, heat-stabilized polyphthalamide (PPA) with a high heat deflection temperature and very high tensile strength. Excellent creep resistance, low mo..
Tensile Strength at Break 275 MPa
39900 psi
Type I, 5 mm/min; ASTM D638
SABIC Innovative Plastics LNP STAT-KON RE007 PA 66
LNP* STAT-KON* RE007 is a compound based on PA66 resin containing 35% Carbon Fiber. Added features include: Electrically Conductive.
Tensile Strength at Break 275 MPa
39900 psi
ISO 527
SABIC Innovative Plastics LNP VERTON UX06451 PPA (Asia Pacific)
LNP* Verton* UX06451 is a compound based on Polyphthalamide resin containing Long Glass Fiber.
Tensile Strength at Break 275 MPa
39900 psi
dry; ISO 527-1/-2
EMS-Grivory Grivory® TSGL-60/4 black 9833 PA666-GF60
Product description: Grilon TSGL-60/4 black is based on a heat stabilized semicrystalline Polyamide PA66+PA6 and 60% long glass fibers. Grilon TSGL-60/4 black is characterized by the following key-p..
Tensile Strength at Break 275 MPa
39900 psi
dry; ISO 527-1/-2
EMS-Grivory Grivory® TSGL-60/4 black 9839 PA666-GF60
Product description: Grilon TSGL-60/4 black 9839 is based on a heat stabilized semi-crystalline Polyamide PA66+PA6 and 60% long glass fibers. Grilon TSGL-60/4 black 9839 is characterized by the foll..
Tensile Strength at Break 275 MPa
39900 psi
ISO 527
Eurotec® Tecomid® NT40 CR30 BK111 HS PPA, 30% carbon fiber reinforced, heat stabilized, natural
Information provided by Eurotec®
Tensile Strength at Break 275 MPa
39900 psi
ISO 527
Eurotec® Tecomid® NT40 GR60 NL HS PPA, 60% glass fiber reinforced, heat stabilized, natural
Information provided by Eurotec®
Tensile Strength at Break 275 MPa
39900 psi
conditioned; ISO 527-1/-2
EMS-Grivory Grivory® GV XE 16102 (GVL-6H HP) PA*-GF60
Product description: Grivory XE 16102 natural is based on a combination of a heat stabilized semi-crystalline Polyamide with a partially aromatic Polyamide and 60% long special glass fibers. Grivory..
Tensile Strength at Break 275 MPa
39900 psi
dry; ISO 527-1/-2
EMS-Grivory Grivory® HT2C-3X black 9833 PA6T/66-CF30
Product description: Grivory HT2C-3X black 9833 us a 30% carbon-fiber reinforced engineering thermoplastic material based on a semi-crystalline, partially aromatic copolyamide. Acc to ISO: PA 6T/66...
Tensile Strength at Break 275 MPa
39900 psi
5 [mm/min]; ISO 527-1/2
Akro-Plastic Akroloy® PA GF 60 (2844) PA 6.6 & PA6I/6T Dry, 60% Glass Filled
One of the most characteristic properties of polyamide (PA 6.6) is the absorption of moisture. This essentially leads to increased toughness and elongation at break, to name the most important param..
Tensile Strength at Break 275 MPa
39900 psi
ISO 527
SABIC Innovative Plastics LNP Verton UX06451 PPA
LNP* Verton* UX06451 is a compound based on Polyphthalamide resin containing Long Glass Fiber.This data was supplied by SABIC-IP for the Americas region.
Tensile Strength at Break 275 MPa
39900 psi
ISO 527
SABIC Innovative Plastics LNP VERTON UX06451 PPA (Europe-Africa-Middle East)
LNP* Verton* UX06451 is a compound based on Polyphthalamide resin containing Long Glass Fiber.
Tensile Strength at Break 275 MPa
39900 psi
5 mm/min; ISO 527
SABIC Innovative Plastics LNP VERTON RX06097 PA 66 (Europe-Africa-Middle East)
LNP* VERTON* RX06097 is a compound based on PA 66 resin containing Long Glass Fiber. Added features include; Easy Molding, UV-Stabilized.