Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Tensile Strength at Break | 3.03 MPa @Temperature 23.0 °C |
439 psi @Temperature 73.4 °F |
Die C2 hr; ASTM D412 |
PolyOne Dynaflex™ G2730 Thermoplastic Elastomer (TPE) Dynaflex™ G2730 is a soft, easy processing compound. - Excellent Weatherability - High Resilience - Soft, Rubbery FeelColor concentrates with polypropylene, ethylene vinyl acetate, or low density p.. |
|||
Tensile Strength at Break | 3.03 MPa | 440 psi | ASTM D638 |
ExxonMobil Escorene™ AD 0428EM1 Ethylene Vinyl Acetate Copolymer (European Grade) Product Description: AD 0428EM1 is a copolymer of ethylene and vinyl acetate.Availability: Africa & Middle East and Europe Additive: Antiblock: NoSlip: NoThermal Stabilizer: YesFree Flowing Agent: .. |
|||
Tensile Strength at Break | 3.03 MPa | 440 psi | ASTM D638 |
ExxonMobil Escorene™ LD 783.CD Ethylene Vinyl Acetate Copolymer Product Description: Escorene Ultra LD 783.CD is a 31.4% VA copolymer that is suitable for making a variety of specialty molding and extrusion compounds. It has high clarity and very low modulus. L.. |
|||
Tensile Strength at Break | 3.03 MPa | 440 psi | ASTM D638 |
ExxonMobil HDPE HD 6909.19 High Density Polyethylene Copolymer Resin Product Description: HD 6908 is a homopolymer with outstanding stiffness with a good balance of processability and cold temperature impact performance. This resin is ideally suited for articles requ.. |
|||
Tensile Strength at Break | 3.03 MPa | 440 psi | ASTM D638 |
ExxonMobil HDPE HD 6909.65 High Density Polyethylene Copolymer Resin Product Description: HD 6908 is a homopolymer with outstanding stiffness with a good balance of processability and cold temperature impact performance. This resin is ideally suited for articles requ.. |
|||
Tensile Strength at Break | 3.03 MPa | 440 psi | ASTM D638 |
ExxonMobil Escorene® UL 7840E Adhesive Application Resin Escorene Ultra UL 7840E is a 31.4% vinyl acetate copolymer that has good compatibility with both hydrocarbon and natural tackifiers and is suitable for making hot melt adhesives adn sealants. UL 784.. |
|||
Tensile Strength at Break | 3.03 MPa | 440 psi | ASTM D638 |
ExxonMobil Escorene® LD 783.ND Molding, extrusion and compounding resin
(discontinued **) Escorene Ultra LD 783.ND is a 33% vinyl acetate copolymer suitable for making a variety of specialty molding and extrusion compounds. It has high clarity and a very low modulus.Information provided .. |