Songhan Plastic Technology Co.,Ltd.
 POLYMER SEARCH

ExxonMobil Escorene® LD 783.ND Molding, extrusion and compounding resin  (discontinued **)

Category Polymer , Thermoplastic , Ethylene Vinyl Acetate , Ethylene Vinyl Acetate Copolymer (EVA), Extrusion/Coating Grade
Manufacturer
Trade Name
Port Ningbo port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF ExxonMobil Escorene® LD 783.ND Molding, extrusion and compounding resin  (discontinued **).pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
Escorene Ultra LD 783.ND is a 33% vinyl acetate copolymer suitable for making a variety of specialty molding and extrusion compounds. It has high clarity and a very low modulus.Information provided by ExxonMobil Chemical
Physical Properties Metric English Comments
Density 0.955 g/cc
0.0345 lb/in³
ExxonMobil Method
Vinyl Acetate Content 33 %
33 %
ExxonMobil Method
Melt Flow 43 g/10 min
43 g/10 min
ASTM D1238
Mechanical Properties Metric English Comments
Hardness, Shore A 55
55
15s; ASTM D2240
Tensile Strength at Break 3.03 MPa
440 psi
ASTM D638
Elongation at Break >= 800 %
>= 800 %
ASTM D638
Flexural Modulus 0.0125 GPa
1.82 ksi
1% secant; ASTM D790
Impact Test 10.8 J

@Temperature 23.0 °C
8.00 ft-lb

@Temperature 73.4 °F
Instrument Impact, Total Energy; ASTM D3763
29.8 J

@Temperature -40.0 °C
22.0 ft-lb

@Temperature -40.0 °F
Instrumented Impact, Total Energy; ASTM D3763
Thermal Properties Metric English Comments
Melting Point 57.8 °C
136 °F
Peak Melting Temperature; ExxonMobil Method
Descriptive Properties Value Comments
Features Thermal Stabilizer