Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Tensile Strength at Break | 3.03 MPa @Temperature 23.0 °C |
439 psi @Temperature 73.4 °F |
Die C2 hr; ASTM D412 |
PolyOne Dynaflex™ G2730 Thermoplastic Elastomer (TPE) Dynaflex™ G2730 is a soft, easy processing compound. - Excellent Weatherability - High Resilience - Soft, Rubbery FeelColor concentrates with polypropylene, ethylene vinyl acetate, or low density p.. |