Mechanical Properties Metric English Comments
Tensile Strength at Break 187 MPa
27100 psi
ISO 527
Nilit FRIANYL A63 HH-GV40 Nylon 6.6 for injection molding, 40% glass fiber reinforced
Nylon 6.6 for injection molding, heat and hydrolysis stabilized.Information provided by Frisetta Polymer, which merged into Nilit Plastics
Tensile Strength at Break 187 MPa

@Temperature 23.0 °C
27100 psi

@Temperature 73.4 °F
DAM; ISO 527
DuPont Performance Polymers Zytel® HTN 52G35HSL BK083 Polyphthalamide (PPA)  (Unverified Data**)
Zytel® HTN52G35HSL BK083 is a 35% glass reinforced, heat stabilized, lubricated high performance polyamide resin that can be molded in water heated molds. It is also a PPA resin.Information provid..
Tensile Strength at Break 187 MPa
27100 psi
Type I, 5.1 mm/min; ASTM D638
PolyOne Nymax™ GF 1200 A 40 IM Black 13A Polyamide 66 (Nylon 66)
The Nymax® GF 1200 Series of glass fiber-reinforced nylon 6/6 compounds have been specifically formulated for applications requiring high stiffness, tensile properties, heat resistance, and durabil..
Tensile Strength at Break 187 MPa
27100 psi
ISO 527-2
Solvay Specialty Polymers Amodel® A-1130 FW Polyphthalamide (PPA)  (Unverified Data**)
Amodel A-1130 FW is a 30% glass-fiber reinforced polyphthalamide (PPA) grade containing a solid lubricant. This resin was designed for moderate-pressure, low-velocity friction and wear applications...
Tensile Strength at Break 187 MPa
27100 psi
ISO 527
SABIC Innovative Plastics LNP LUBRICOMP LCL33 PEEK
LNP* LUBRICOMP* LCL33 is a compound based on Polyetheretherketone resin containing 15% Carbon Fiber, 15% PTFE. Added features of this material include: Wear Resistant.
Tensile Strength at Break 187 MPa
27100 psi
ISO 527
SABIC Innovative Plastics LNP LUBRICOMP LCL33E PEEK
LNP LUBRICOMP* LCL33E is a compound based on Polyetheretherketone resin containing 15% Carbon Fiber, 15% PTFE. Added features of this material include: Easy Molding, Wear Resistant.
Tensile Strength at Break 187 MPa
27100 psi
ISO 527-2
Solvay Specialty Polymers Amodel® A-1130 FW Polyphthalamide (PPA), 30% Glass Fiber
Amodel® A-1130 FW is a 30% glass-fiber reinforced polyphthalamide (PPA) grade containing a solid lubricant. This resin was designed for moderate-pressure, low-velocity friction and wear applicati..
Tensile Strength at Break 187 MPa
27100 psi
ISO 527
SABIC Innovative Plastics LNP THERMOCOMP LF006E PEEK
LNP* THERMOCOMP* LF006E is a compound based on Polyetheretherketone resin containing 30% Glass Fiber. Added features of this material include: Easy Molding.
Tensile Strength at Break 187 MPa
27100 psi
Type I, 5 mm/min; ASTM D638
SABIC Innovative Plastics LNP VERTON EV008 PEI
LNP* VERTON* EV008 is a compound based on Polyetherimide containing 40% Long Glass Fiber. Added feature of this grade is: Structural.
Tensile Strength at Break 187 MPa
27100 psi
ISO 527
SABIC Innovative Plastics LNP VERTON WV006 PBT (Europe-Africa-Middle East)
LNP VERTON* WV006 is a compound based on Polybutylene Terephalate resin containing Long Glass.
Tensile Strength at Break 187 MPa

@Temperature 23.0 °C
27100 psi

@Temperature 73.4 °F
DAM; ISO 527
DuPont Performance Polymers Zytel® HTN 54G35EF NC010 Polyphthalamide (PPA)
Zytel® HTN54G35EF NC010 is a 35% glass reinforced, toughened, heat stabilized, lubricated high performance polyamide resin, developed for electrical and electronics applications. It is also a PPA r..
Tensile Strength at Break 187 MPa
27100 psi
DAM; ISO 527-1/-2
DuPont Performance Polymers Zytel® HTN 52G35HSL BK083 Polyphthalamide (PPA)  (Unverified Data**)
35% Glass Reinforced PPA High Performance Polyamide Zytel HTN52G35HSL BK083 is a 35% glass reinforced heat stabilized lubricated high performance polyamide resin that can be molded in water heated m..