Songhan Plastic Technology Co.,Ltd.
 POLYMER SEARCH

Solvay Specialty Polymers Amodel® A-1130 FW Polyphthalamide (PPA)  (Unverified Data**)

Category Polymer , Thermoplastic , Polyphthalamide (PPA) , Polyphthalamide (PPA), 30% Glass Fiber Reinforced
Manufacturer
Trade Name
Port Shanghai port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF Solvay Specialty Polymers Amodel® A-1130 FW Polyphthalamide (PPA)  (Unverified Data**).pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
Amodel A-1130 FW is a 30% glass-fiber reinforced polyphthalamide (PPA) grade containing a solid lubricant. This resin was designed for moderate-pressure, low-velocity friction and wear applications. - Black: A-1130 FW BK 324Information provided by Solvay Specialty Polymers.
Physical Properties Metric English Comments
Density 1.55 g/cc
0.0560 lb/in³
ISO 1183/A
Filler Content 30 %
30 %
Glass Fiber Reinforcement
Mechanical Properties Metric English Comments
Tensile Strength at Break 187 MPa
27100 psi
ISO 527-2
Elongation at Break 2.0 %
2.0 %
ISO 527-2
Tensile Modulus 11.2 GPa
1620 ksi
ISO 527-2
Flexural Strength 252 MPa
36500 psi
ISO 178
Flexural Modulus 9.58 GPa
1390 ksi
ISO 178
Thermal Properties Metric English Comments
Melting Point 313 °C
595 °F
ISO 11357-3
Deflection Temperature at 1.8 MPa (264 psi) 285 °C
545 °F
Unannealed; ISO 75-2/A
Processing Properties Metric English Comments
Rear Barrel Temperature 304 - 318 °C
579 - 604 °F
Front Barrel Temperature 316 - 329 °C
601 - 624 °F
Melt Temperature 329 - 343 °C
624 - 649 °F
Mold Temperature 135 °C
275 °F
Drying Temperature 110 °C
230 °F
Dry Time 4.00 hour
4.00 hour
Moisture Content 0.045 %
0.045 %
Descriptive Properties Value Comments
Additive PTFE Lubricant
Appearance Black
Automotive Specifications ASTM D6779 PA1270G30
ISO 1874-PA6T/6I/66, MH, 11-110, GF30
Availability Africa & Middle East
Asia Pacific
Europe
North America
South America
Features Good Chemical Resistance
Good Creep Resistance
Good Dimensional Stability
Good Stiffness
Good Wear Resistance
High Strength
Low Friction
Forms Pellets
Generic PPA
Processing Method Injection Molding
RoHS Compliance RoHS Compliant
Uses Bearings
Bushings
Filters
Gears