Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Tensile Strength at Break | 9.65 MPa | 1400 psi | ASTM D412 |
Noble Polymers Ecobarrier™ 2614 Thermoplastic Olefin (TPO) Ecobarrier is a TPO (thermoplastic olefin) produced by Noble Polymers based on olefin/elastomer compounding. Ecobarrier is primarily used as a sound barrier material in low heat applications.Informa.. |
|||
Tensile Strength at Break | 9.65 MPa | 1400 psi | 510 mm/min; ASTM D412A |
PolyOne Elastamax™ TM0200-0085 Black Thermoplastic Polyolefin Elastomer (TPO (POE)) PolyOne's Elastamax™ XL thermoplastic olefins (TPOs) are based on pelletized blends of polyolefin resins and select elastomers such EPDM. These materials have been engineered to provide a balance o.. |
|||
Tensile Strength at Break | 9.65 MPa | 1400 psi | ASTM D638 |
ExxonMobil LD 503.LN Foams and Compounding Resin
(discontinued **) LD 503.LN is a low density homopolymer specially designed for maximum performance in foam applications.Information provided by ExxonMobil Chemical |
|||
Tensile Strength at Break | 9.65 MPa | 1400 psi | |
Indium Corp. Indalloy® 131 97Sn/3Sb Lead-Free Solder Alloy Information provided by the manufacturer, Indium Corporation. |
|||
Tensile Strength at Break | 9.65 MPa | 1400 psi | DBPH Cure |
Shin-Etsu Silicones SV-55002U High Strength Silicone Elastomer SV55002U is one of a series of silicone bases Type of HCR designed for applications requiring high strength. Product Features: Excellent mechanical properties.Typical Applications: Molding and Extru.. |
|||
Tensile Strength at Break | 9.64 MPa | 1400 psi | ISO R 527 |
Stir SpA CT 45 ATC (PVC) Application: Transparent inner soleInformation provided by STIR SpA |
|||
Tensile Strength at Break | 9.65 MPa | 1400 psi | ASTM D638 |
Teknor Apex APEX® 3800-60 Polyvinyl Chloride, Flexible Features: DEHP Plasticizer; Ethylene Oxide Sterilizable; High Heat Resistance Uses: Medical/Healthcare Applications Processing Method: Injection Molding Forms: PelletsInformation Provided by Teknor .. |
|||
Tensile Strength at Break | 9.65 MPa | 1400 psi | ASTM D412 |
Teknor Apex Monprene® MP 1093L Thermoplastic Elastomer Uses: Closures; Consumer Applications; Gaskets; Handles; Kitchenware; Medical/Healthcare Applications; Packaging; Safety Equipment; Sporting Goods; Toothbrush Handles; Tubing; Writing Instruments Fo.. |
|||
Tensile Strength at Break | 9.65 MPa | 1400 psi | ASTM D412 |
Teknor Apex Monprene® MP 1097D Thermoplastic Elastomer Uses: Closures; Consumer Applications; Gaskets; Handles; Kitchenware; Medical/Healthcare Applications; Packaging; Safety Equipment; Sporting Goods; Toothbrush Handles; Tubing; Writing Instruments Fo.. |
|||
Tensile Strength at Break | 9.65 MPa | 1400 psi | ASTM D412 |
Teknor Apex Monprene® MP 2860E Thermoplastic Elastomer Notes: Translucent Features: Good Chemical and Oil Resistance; Tough; Good Melt StrengthInformation Provided by Teknor Apex |
|||
Tensile Strength at Break | 9.65 MPa | 1400 psi | ASTM D412 |
Teknor Apex Monprene® MP-1564F Thermoplastic Elastomer Uses: Closures; Consumer Applications; Gaskets; Handles; Kitchenware; Medical/Healthcare Applications; Packaging; Safety Equipment; Sporting Goods; Toothbrush Handles; Tubing; Writing Instruments Fo.. |
|||
Tensile Strength at Break | 9.65 MPa | 1400 psi | ASTM D412 |
Teknor Apex Monprene® MP-1658A Thermoplastic Elastomer Uses: Closures; Consumer Applications; Gaskets; Handles; Kitchenware; Medical/Healthcare Applications; Packaging; Safety Equipment; Sporting Goods; Toothbrush Handles; Tubing; Writing Instruments Fo.. |
|||
Tensile Strength at Break | 9.65 MPa | 1400 psi | ASTM D412 |
Teknor Apex Monprene® MP-1743UV Thermoplastic Elastomer Uses: Closures; Consumer Applications; Gaskets; Handles; Kitchenware; Medical/Healthcare Applications; Packaging; Safety Equipment; Sporting Goods; Toothbrush Handles; Tubing; Writing Instruments Fo.. |
|||
Tensile Strength at Break | 9.65 MPa | 1400 psi | ASTM D412 |
Teknor Apex Monprene® MP-1766 Thermoplastic Elastomer Uses: Closures; Consumer Applications; Gaskets; Handles; Kitchenware; Medical/Healthcare Applications; Packaging; Safety Equipment; Sporting Goods; Toothbrush Handles; Tubing; Writing Instruments Fo.. |
|||
Tensile Strength at Break | 9.65 MPa | 1400 psi | ASTM D412 |
Teknor Apex Monprene® MP-2249 Thermoplastic Elastomer Uses: Closures; Consumer Applications; Gaskets; Handles; Kitchenware; Medical/Healthcare Applications; Packaging; Safety Equipment; Sporting Goods; Toothbrush Handles; Tubing; Writing Instruments Fo.. |
|||
Tensile Strength at Break | 9.66 MPa | 1400 psi | ISO R 527 |
Stir SpA Z 52 AT (PVC) Application: Foamed intersoleInformation provided by STIR SpA |
|||
Tensile Strength at Break | 9.65 MPa | 1400 psi | ASTM D412 |
Teknor Apex Monprene® MP-1855PV2 Thermoplastic Elastomer Uses: Closures; Consumer Applications; Gaskets; Handles; Kitchenware; Medical/Healthcare Applications; Packaging; Safety Equipment; Sporting Goods; Toothbrush Handles; Tubing; Writing Instruments Fo.. |
|||
Tensile Strength at Break | 9.65 MPa | 1400 psi | ASTM D412 |
Teknor Apex Monprene® MP-2790 Thermoplastic Elastomer Uses: Closures; Consumer Applications; Gaskets; Handles; Kitchenware; Medical/Healthcare Applications; Packaging; Safety Equipment; Sporting Goods; Toothbrush Handles; Tubing; Writing Instruments Fo.. |
|||
Tensile Strength at Break | 9.65 MPa | 1400 psi | 20 in/min; ASTM D412 |
Teknor Apex Telcar® TL-1934G Styrenic Thermoplastic Elastomer Notes: RoHS Compliant Uses: Appliance Wire Insulation; Cable Jacketing; Flexible Cord Insulation; Connectors; Wire Jacketing; Wire and Cable Applications Agency Ratings: UL 1581Forms: Pellets Proces.. |
|||
Tensile Strength at Break | 9.65 MPa | 1400 psi | ASTM D412 |
Teknor Apex Telcar® TL-4001 Thermoplastic Elastomer Uses: Automotive Applications; Automotive Exterior Parts; Automotive Exterior Trim; Automotive Interior Parts; Blow Molding Applications; General Purpose; Grommets; Weatherstripping Forms: Pellets .. |
|||
Tensile Strength at Break | 9.65 MPa | 1400 psi | ASTM D638 |
ExxonMobil Escorene® LD 768.MJ Molding, extrusion and compounding resin Escorene Ultra LD 768.MJ is a high viscosity, 26.2% vinyl acetate copolymer suitable for making very soft, blow molded or extruded articles with very good low temperature toughness. It can also be .. |
|||
Tensile Strength at Break | 9.65 MPa | 1400 psi | ASTM D638 |
ExxonMobil Escorene™ LD 727.22 Ethylene Vinyl Acetate Copolymer Product Description: Escorene Ultra LD 727.22 is a high vinyl acetate copolymer with a low melting temperature and excellent strength properties and toughness.Availability: North America Additive: .. |
|||
Tensile Strength at Break | 9.65 MPa | 1400 psi | ASTM D638 |
ExxonMobil LDPE LD 503.LP Low Density Polyethylene Resin Product Description: LD 503.LP is a LDPE homopolymer that is suitable for use in molding, extrusion, compounding and foam applications.Availability: Latin America, North America and South AmericaAdd.. |
|||
Tensile Strength at Break | 9.65 MPa | 1400 psi | Molded and tested in accordance with ASTM D4976; ASTM D638 |
Dow 722 Linear Low Density Polyethylene (LDPE) DOW Polyethylene 722 is a broad molecular weight distribution homopolymer designed to offer good impact strength and rack resistance, with excellent flexibility. Typical applications include caps/c.. |
|||
Tensile Strength at Break | 9.65 MPa | 1400 psi | ASTM D412 |
Teknor Apex Monprene® MP-2579B Thermoplastic Elastomer Uses: Closures; Consumer Applications; Gaskets; Handles; Kitchenware; Medical/Healthcare Applications; Packaging; Safety Equipment; Sporting Goods; Toothbrush Handles; Tubing; Writing Instruments Fo.. |
|||
Tensile Strength at Break | 9.65 MPa | 1400 psi | Type IV, 510 mm/min; ASTM D638 |
PolyOne Geon™ Vinyl Wire & Cable JA508AF Polyvinyl Chloride, Flexible (PVC, Flexible) Typical Properties of Molded Slab (0.075); Not to be Construed as Specifications.Information provided by PolyOne |
|||
Tensile Strength at Break | 9.65 MPa | 1400 psi | ASTM D412 |
Teknor Apex Monprene® MP 1210A Thermoplastic Elastomer Uses: Closures; Consumer Applications; Gaskets; Handles; Kitchenware; Medical/Healthcare Applications; Packaging; Safety Equipment; Sporting Goods; Toothbrush Handles; Tubing; Writing Instruments Fo.. |