Songhan Plastic Technology Co.,Ltd.
 POLYMER SEARCH

ExxonMobil LD 503.LN Foams and Compounding Resin  (discontinued **)

Category Polymer , Thermoplastic , Polyethylene (PE) , LDPE , Low Density Polyethylene (LDPE), Molded
Manufacturer
Trade Name
Port Shanghai port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF ExxonMobil LD 503.LN Foams and Compounding Resin  (discontinued **).pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
LD 503.LN is a low density homopolymer specially designed for maximum performance in foam applications.Information provided by ExxonMobil Chemical
Physical Properties Metric English Comments
Density 0.918 g/cc
0.0332 lb/in³
ExxonMobil Method
Melt Flow 2.3 g/10 min
2.3 g/10 min
ExxonMobil Method
Mechanical Properties Metric English Comments
Hardness, Shore A 84
84
15s; ASTM D2240
Hardness, Shore D 48
48
15s; ASTM D2240
Tensile Strength at Break 9.65 MPa
1400 psi
ASTM D638
Tensile Strength, Yield 10.3 MPa
1500 psi
at 2% Offset; ASTM D638
Elongation at Break >= 800 %
>= 800 %
ASTM D638
Elongation at Yield 33 %
33 %
ASTM D638
1% Secant Modulus 207 MPa
30000 psi
ASTM D790
Impact Test 9.90 - 18.0 J
7.30 - 13.3 ft-lb
Instrumented Impact Total Energy; ASTM D3763
15.5 - 24.5 J

@Temperature -20.0 °C
11.4 - 18.1 ft-lb

@Temperature -4.00 °F
Instrumented Impact Total Energy; ASTM D3763
Thermal Properties Metric English Comments
Melting Point 110 °C
230 °F
Peak Melting Temperature; ExxonMobil Method
Vicat Softening Point 86.7 °C
188 °F
ASTM D1525
Copyright © lookpolymers.com All Rights Reserved