Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Tensile Strength at Break | 9.65 MPa | 1400 psi | ASTM D412 |
Noble Polymers Ecobarrier™ 2614 Thermoplastic Olefin (TPO) Ecobarrier is a TPO (thermoplastic olefin) produced by Noble Polymers based on olefin/elastomer compounding. Ecobarrier is primarily used as a sound barrier material in low heat applications.Informa.. |
|||
Tensile Strength at Break | 9.65 MPa | 1400 psi | 510 mm/min; ASTM D412A |
PolyOne Elastamax™ TM0200-0085 Black Thermoplastic Polyolefin Elastomer (TPO (POE)) PolyOne's Elastamax™ XL thermoplastic olefins (TPOs) are based on pelletized blends of polyolefin resins and select elastomers such EPDM. These materials have been engineered to provide a balance o.. |
|||
Tensile Strength at Break | 9.65 MPa | 1400 psi | 510 mm/min; ASTM D638 |
PolyOne Geon™ Vinyl Flexible A6500 Polyvinyl Chloride, Flexible (PVC, Flexible) Recommended for interior applications.Information provided by PolyOne |
|||
Tensile Strength at Break | 9.65 MPa | 1400 psi | 510 mm/min; ASTM D638 |
PolyOne Geon™ Vinyl Flexible B65B0 Polyvinyl Chloride, Flexible (PVC, Flexible) Information provided by PolyOne |
|||
Tensile Strength at Break | 9.65 MPa | 1400 psi | 510 mm/min; ASTM D638 |
PolyOne Geon™ Vinyl Flexible C70A0 Polyvinyl Chloride, Flexible (PVC, Flexible) Information provided by PolyOne |
|||
Tensile Strength at Break | 9.65 MPa | 1400 psi | Type IV, 510 mm/min; ASTM D638 |
PolyOne Geon™ Vinyl Flexible C70UB Polyvinyl Chloride, Flexible (PVC, Flexible) Information provided by PolyOne |
|||
Tensile Strength at Break | 9.65 MPa | 1400 psi | |
Indium Corp. Indalloy® 131 97Sn/3Sb Lead-Free Solder Alloy Information provided by the manufacturer, Indium Corporation. |
|||
Tensile Strength at Break | 9.65 MPa | 1400 psi | DBPH Cure |
Shin-Etsu Silicones SV-55002U High Strength Silicone Elastomer SV55002U is one of a series of silicone bases Type of HCR designed for applications requiring high strength. Product Features: Excellent mechanical properties.Typical Applications: Molding and Extru.. |
|||
Tensile Strength at Break | 9.65 MPa | 1400 psi | ASTM D638 |
Teknor Apex APEX® 3800-60 Polyvinyl Chloride, Flexible Features: DEHP Plasticizer; Ethylene Oxide Sterilizable; High Heat Resistance Uses: Medical/Healthcare Applications Processing Method: Injection Molding Forms: PelletsInformation Provided by Teknor .. |
|||
Tensile Strength at Break | 9.65 MPa | 1400 psi | ASTM D412 |
Teknor Apex Monprene® MP 1097D Thermoplastic Elastomer Uses: Closures; Consumer Applications; Gaskets; Handles; Kitchenware; Medical/Healthcare Applications; Packaging; Safety Equipment; Sporting Goods; Toothbrush Handles; Tubing; Writing Instruments Fo.. |
|||
Tensile Strength at Break | 9.65 MPa | 1400 psi | ASTM D412 |
Teknor Apex Monprene® MP 1643L1 Thermoplastic Elastomer Notes: Translucent Features: Tough; Good Melt StrengthInformation Provided by Teknor Apex |
|||
Tensile Strength at Break | 9.65 MPa | 1400 psi | ASTM D412 |
Teknor Apex Monprene® MP-1743UV Thermoplastic Elastomer Uses: Closures; Consumer Applications; Gaskets; Handles; Kitchenware; Medical/Healthcare Applications; Packaging; Safety Equipment; Sporting Goods; Toothbrush Handles; Tubing; Writing Instruments Fo.. |
|||
Tensile Strength at Break | 9.65 MPa | 1400 psi | ASTM D412 |
Teknor Apex Monprene® MP-1766 Thermoplastic Elastomer Uses: Closures; Consumer Applications; Gaskets; Handles; Kitchenware; Medical/Healthcare Applications; Packaging; Safety Equipment; Sporting Goods; Toothbrush Handles; Tubing; Writing Instruments Fo.. |
|||
Tensile Strength at Break | 9.65 MPa | 1400 psi | ASTM D412 |
Teknor Apex Monprene® MP-2249 Thermoplastic Elastomer Uses: Closures; Consumer Applications; Gaskets; Handles; Kitchenware; Medical/Healthcare Applications; Packaging; Safety Equipment; Sporting Goods; Toothbrush Handles; Tubing; Writing Instruments Fo.. |
|||
Tensile Strength at Break | 9.65 MPa | 1400 psi | ASTM D412 |
Teknor Apex Monprene® MP-2790 Thermoplastic Elastomer Uses: Closures; Consumer Applications; Gaskets; Handles; Kitchenware; Medical/Healthcare Applications; Packaging; Safety Equipment; Sporting Goods; Toothbrush Handles; Tubing; Writing Instruments Fo.. |
|||
Tensile Strength at Break | 9.65 MPa | 1400 psi | ASTM D412 |
Teknor Apex Telcar® TL-2519G Thermoplastic Elastomer Uses: Automotive Applications; Automotive Exterior Parts; Automotive Exterior Trim; Automotive Interior Parts; Blow Molding Applications; General Purpose; Grommets; Weatherstripping Forms: Pellets .. |
|||
Tensile Strength at Break | 9.65 MPa | 1400 psi | ASTM D412 |
Teknor Apex Telcar® TL-4001 Thermoplastic Elastomer Uses: Automotive Applications; Automotive Exterior Parts; Automotive Exterior Trim; Automotive Interior Parts; Blow Molding Applications; General Purpose; Grommets; Weatherstripping Forms: Pellets .. |
|||
Tensile Strength at Break | 9.65 MPa | 1400 psi | ASTM D412 |
Teknor Apex Telcar® TL-4002 Thermoplastic Elastomer Uses: Automotive Applications; Automotive Exterior Parts; Automotive Exterior Trim; Automotive Interior Parts; Blow Molding Applications; General Purpose; Grommets; Weatherstripping Forms: Pellets .. |
|||
Tensile Strength at Break | 9.65 MPa | 1400 psi | ASTM D638 |
ExxonMobil Escorene® LD 768.MJ Molding, extrusion and compounding resin Escorene Ultra LD 768.MJ is a high viscosity, 26.2% vinyl acetate copolymer suitable for making very soft, blow molded or extruded articles with very good low temperature toughness. It can also be .. |
|||
Tensile Strength at Break | 9.65 MPa | 1400 psi | ASTM D638 |
ExxonMobil LDPE LD 503.LP Low Density Polyethylene Resin Product Description: LD 503.LP is a LDPE homopolymer that is suitable for use in molding, extrusion, compounding and foam applications.Availability: Latin America, North America and South AmericaAdd.. |
|||
Tensile Strength at Break | 9.65 MPa | 1400 psi | Molded and tested in accordance with ASTM D4976; ASTM D638 |
Dow 722 Linear Low Density Polyethylene (LDPE) DOW Polyethylene 722 is a broad molecular weight distribution homopolymer designed to offer good impact strength and rack resistance, with excellent flexibility. Typical applications include caps/c.. |
|||
Tensile Strength at Break | 9.65 MPa | 1400 psi | Compression molded; ASTM D638 |
Dow Primacor® 5986 Ethylene acrylic acid copolymer Low heat seal temperature High gloss, excellent clarity Excellent grease and oil resistance and excellent product resistance for flexible packaging applications Complies with U.S. FDA 21 CFR 177.131.. |
|||
Tensile Strength at Break | 9.65 MPa | 1400 psi | ASTM D412 |
Compuestos Dominicanos Polycom CQ-000365 PVC Compound Compuestos Dominicanos SA produces a wide variety of PVC compounds for the injection molding of footwear products; everything from full injection, shoe soles, boots, and PVC compounds for oil resist.. |
|||
Tensile Strength at Break | 9.65 MPa | 1400 psi | ASTM D412 |
Teknor Apex Monprene® MP-2579B Thermoplastic Elastomer Uses: Closures; Consumer Applications; Gaskets; Handles; Kitchenware; Medical/Healthcare Applications; Packaging; Safety Equipment; Sporting Goods; Toothbrush Handles; Tubing; Writing Instruments Fo.. |
|||
Tensile Strength at Break | 9.65 MPa | 1400 psi | Type IV, 510 mm/min; ASTM D638 |
PolyOne Geon™ Vinyl Wire & Cable JA508AF Polyvinyl Chloride, Flexible (PVC, Flexible) Typical Properties of Molded Slab (0.075); Not to be Construed as Specifications.Information provided by PolyOne |