Material Notes:
Scotch® 24 Electrical Shielding Tape is an all-metal, open-weave, shielding braid tape in a flat, cable-like form. It is conformable due to the open-weave knit construction of two No. AWG tinned copper wires.Information provided by 3M
Physical Properties Metric English Comments
Thickness 406 microns
16.0 mil
Mechanical Properties Metric English Comments
Tensile Strength at Break 9.37 MPa
1360 psi
ASTM D1000
Elongation at Break 70 %
70 %
ASTM D1000
Users viewing this material also viewed the following: