Mechanical Properties Metric English Comments
Izod Impact, Unnotched 7.40 J/cm

@Thickness 4.00 mm,
Temperature 23.0 °C
13.9 ft-lb/in

@Thickness 0.157 in,
Temperature 73.4 °F
ISO 180
Premix Thermoplastics PRE-ELEC® 12-000
PRE-ELEC 12-000 is a conductive thermoplastic compound based on a polyacetal copolymer. Conductivity is achieved by using special carbon black. In addition to a low resistivity PRE-ELEC 12-000 has a..
Izod Impact, Unnotched 7.40 J/cm
13.9 ft-lb/in
ASTM D4812
SABIC Innovative Plastics LNP LUBRICOMP DFL34EH PC
LNP* LUBRICOMP* DFL34EH is a compound based on Polycarbonate containing 20% Glass Fiber, 15% PTFE. Added features of this material include: Easy Molding, Healthcare, Wear Resistant.
Izod Impact, Unnotched 7.40 J/cm
13.9 ft-lb/in
ASTM Test
BASF Ultramid® 8267G HS BK-102 15/25% Glass/Mineral Filled PA6 (Dry)
Ultramid 8267G HS BK-102 is a heat stabilized, black pigmented, 40% mineral and glass fiber reinforced nylon 6 injection molding compound. It possesses a balance of engineering properties in combin..