Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Izod Impact, Unnotched | 7.40 J/cm @Thickness 4.00 mm, Temperature 23.0 °C |
13.9 ft-lb/in @Thickness 0.157 in, Temperature 73.4 °F |
ISO 180 |
Premix Thermoplastics PRE-ELEC® 12-000 PRE-ELEC 12-000 is a conductive thermoplastic compound based on a polyacetal copolymer. Conductivity is achieved by using special carbon black. In addition to a low resistivity PRE-ELEC 12-000 has a.. |
|||
Izod Impact, Unnotched | 7.40 J/cm | 13.9 ft-lb/in | ASTM D4812 |
SABIC Innovative Plastics LNP LUBRICOMP DFL34EH PC LNP* LUBRICOMP* DFL34EH is a compound based on Polycarbonate containing 20% Glass Fiber, 15% PTFE. Added features of this material include: Easy Molding, Healthcare, Wear Resistant. |
|||
Izod Impact, Unnotched | 7.42 J/cm | 13.9 ft-lb/in | ASTM D4812 |
SABIC Innovative Plastics LNP LUBRICOMP RAL22 PA 66 LNP LUBRICOMP* RAL22 is a compound based on Nylon 66 resin containing 10% PTFE, 10% Aramid. Added features of this material include: Wear Resistant. |
|||
Izod Impact, Unnotched | 7.42 J/cm | 13.9 ft-lb/in | ASTM D4812 |
SABIC Innovative Plastics LNP LUBRICOMP RAL22 PA 66 (Asia Pacific) LNP LUBRICOMP* RAL22 is a compound based on Nylon 66 resin containing Aramid, PTFE. Added features of this material include: Internally Lubricated. |
|||
Izod Impact, Unnotched | 7.42 J/cm | 13.9 ft-lb/in | ASTM D4812 |
SABIC Innovative Plastics LNP LUBRICOMP WFL34H PBT (Asia Pacific) LNP* LUBRICOMP* WFL34H is a compound based on Polybutylene Terephalate resin containing PTFE, Glass Fiber. Added features of this material include: Internally Lubricated. |
|||
Izod Impact, Unnotched | 7.44 J/cm | 13.9 ft-lb/in | ASTM D4812 |
SABIC Innovative Plastics LNP STAT-KON CD0001 PS LNP* STAT-KON* CD000I is a compound based on Polystyrene resin containing Carbon Powder. Added features of this material include: Electrically Conductive, High Impact. |
|||
Izod Impact, Unnotched | 7.44 J/cm | 13.9 ft-lb/in | ASTM D4812 |
SABIC Innovative Plastics LNP STAT-KON CD000I PS LNP* Stat-kon* CD000I is a compound based on Polystyrene resin containing Carbon Powder. Added features of this material include: Electrically Conductive, High Impact. |
|||
Izod Impact, Unnotched | 7.43 J/cm | 13.9 ft-lb/in | ASTM D4812 |
SABIC Innovative Plastics LNP THERMOCOMP DF004P PC (Asia Pacific) LNP* Thermocomp* DF004P is a Polycarbonate base resin containing Glass Fiber. Characteristics of this grade are Exceptional Processing. |
|||
Izod Impact, Unnotched | 7.41 J/cm @Temperature 23.0 °C |
13.9 ft-lb/in @Temperature 73.4 °F |
ASTM D 4812 |
SABIC Innovative Plastics LNP Thermocomp DF0066P PC LNP THERMOCOMP* DF0066P is a compound based on Polycarbonate resin containing Glass Fiber, Flame Retardant. Added features of this material include: Exceptional Processing.This data was supplied by.. |
|||
Izod Impact, Unnotched | 7.42 J/cm @Temperature 23.0 °C |
13.9 ft-lb/in @Temperature 73.4 °F |
ASTM D 4812 |
SABIC Innovative Plastics LNP Verton OX07411 PPS (Asia Pacific) LNP* Verton* OX07411 is a compound based on Polyphenylene Sulfide resin containing Long Glass Fiber.This data was supplied by SABIC-IP for the Asia Pacific region. |
|||
Izod Impact, Unnotched | 7.40 J/cm | 13.9 ft-lb/in | ASTM Test |
BASF Ultramid® 8267G HS BK-102 15/25% Glass/Mineral Filled PA6 (Dry) Ultramid 8267G HS BK-102 is a heat stabilized, black pigmented, 40% mineral and glass fiber reinforced nylon 6 injection molding compound. It possesses a balance of engineering properties in combin.. |
|||
Izod Impact, Unnotched | 7.42 J/cm @Temperature 23.0 °C |
13.9 ft-lb/in @Temperature 73.4 °F |
ASTM D 4812 |
SABIC Innovative Plastics LNP Verton OX07411 PPS LNP* Verton* OX07411 is a compound based on Polyphenylene Sulfide resin containing Long Glass Fiber.This data was supplied by SABIC-IP for the Americas region. |