Mechanical Properties Metric English Comments
Izod Impact, Unnotched 3.31 J/cm
6.20 ft-lb/in
ASTM D4812
SABIC Innovative Plastics Lexan® JK2000 PC+ABS (Asia Pacific)
Lexan* JK2000 compound is a glass reinforced, non-Br and non-Cl FR polycarbonate blends designed for thinwall molding applications.
Izod Impact, Unnotched 3.31 J/cm
6.20 ft-lb/in
ASTM D4812
SABIC Innovative Plastics LNP LUBRICOMP RL0019 PA 66
LNP LUBRICOMP* RL0019 is a compound based on Nylon 66 resin containing 5% PTFE. Added features of this material include: Flame Retardant, Wear Resistant.
Izod Impact, Unnotched 3.31 J/cm
6.20 ft-lb/in
ASTM D4812
SABIC Innovative Plastics LNP THERMOCOMP Lexan_JK2000 PC+ABS
LNP* Thermocomp* Lexan_JK2000 compound is a 22% GR, ECO-compliant FR, PC+ABS for thinwall molding applications.
Izod Impact, Unnotched 3.31 J/cm
6.20 ft-lb/in
ASTM D4812
SABIC Innovative Plastics LNP THERMOCOMP Noryl_PCN2910 PPE+PS
LNP* Thermodcomp* Noryl_PCN2910 compound is a 35% Glass/Mica filled. High modulus and tight tolerance molding for the chassis market.
Izod Impact, Unnotched 3.31 J/cm
6.20 ft-lb/in
ASTM D4812
SABIC Innovative Plastics NORYL PCN2910 PPE+PS (Asia Pacific)
35% Glass/Mica filled. High modulus and tight tolerance molding for the chassis market.
Izod Impact, Unnotched 3.31 J/cm
6.20 ft-lb/in
ASTM D4812
SABIC Innovative Plastics LNP LUBRICOMP JX91198 PES
LNP LUBRICOMP* JX91198 is a compound based on Polyethersulfone resin containing Proprietary Filler(s). Added feature of this material is: Wear Resistant.
Izod Impact, Unnotched 3.31 J/cm
6.20 ft-lb/in
ASTM D4812
SABIC Innovative Plastics LNP THERMOCOMP Noryl_PCN2910 PPE+PS (Asia Pacific)
35% Glass/Mica filled. High modulus and tight tolerance molding for the chassis market.
Izod Impact, Unnotched 3.31 J/cm

@Thickness 3.18 mm
6.20 ft-lb/in

@Thickness 0.125 in
ASTM D256
LNP Lubricomp® PDX-J-91198 Polyethersulfone, Proprietary Filler  (discontinued **)
Features: LubricatedForms: PelletsProcessing Method: Injection MoldingInformation provided by LNP, a GE Plastics Company.This data sheet is labeled Discontinued; however many LNP grades are still ac..