Songhan Plastic Technology Co.,Ltd.
 POLYMER SEARCH

Polymer Property : Izod Impact, Unnotched = 26.7 J/cm Product List

Mechanical Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Mechanical Properties Metric English Comments
Izod Impact, Unnotched 26.7 J/cm
50.0 ft-lb/in
ASTM D4812
SABIC Innovative Plastics FL405 PC
Various weight reductions at 0.250"" (6.38 mm) wall. Impact resistant, superior processing, excellent surface. UL94 V-0 at 0.120
Izod Impact, Unnotched 26.7 J/cm

@Temperature 23.0 °C
50.0 ft-lb/in

@Temperature 73.4 °F
ASTM D 4812
SABIC Innovative Plastics Lexan® FL2003 PC
Various weight reductions at 0.250" (6.35mm) wall. Low temperature impact and high heat resistant. Excellent surface. UV-stabilized.This data was supplied by SABIC-IP for the Americas region.
Izod Impact, Unnotched 26.7 J/cm

@Thickness 6.40 mm
50.0 ft-lb/in

@Thickness 0.252 in
ASTM D4812
SABIC Innovative Plastics Lexan® FL2000 PC
Lexan FL2000 is a medium flow specialty polycarbonate (PC) resin for structural foam molding, allowing for various weight reductions at 0.24"" (6.0mm) wall. This product offers low temperature impa..
Izod Impact, Unnotched 26.7 J/cm

@Temperature 23.0 °C
50.0 ft-lb/in

@Temperature 73.4 °F
ASTM D 4812
SABIC Innovative Plastics Lexan® FL2003 PC (Asia Pacific)
Various weight reductions at 0.250" (6.35mm) wall. Low temperature impact and high heat resistant. Excellent surface. UV-stabilized.This data was supplied by SABIC-IP for the Asia Pacific region...
Izod Impact, Unnotched 26.7 J/cm
50.0 ft-lb/in
ASTM D4812
SABIC Innovative Plastics Lexan® FL403 PC
Various weight reductions at 0.250"" wall. UV-resistant. Impact resistant, Superior processing, excellent surface. UL94 V-0/5V at 0.125"".
Izod Impact, Unnotched 26.7 J/cm
50.0 ft-lb/in
ASTM D4812
SABIC Innovative Plastics Lexan® FL405 PC
Various weight reductions at 0.250"" (6.38 mm) wall. Impact resistant, superior processing, excellent surface. UL94 V-0 at 0.120
Copyright © lookpolymers.com All Rights Reserved