Mechanical Properties Metric English Comments
Izod Impact, Unnotched 2.80 J/cm
5.25 ft-lb/in
ASTM D256
Solvay Specialty Polymers Primef® 7010 Polyphenylene Sulfide (PPS), 65% GlassMineral  (discontinued **)
Primef 7010 is a 65% mineral/glass fiber reinforced polyphenylene sulfide (PPS). This grade offers improved mechanical properties versus Primef 7002 (also 65% mineral/glass fiber), but with less flu..
Izod Impact, Unnotched 2.80 - 3.20 J/cm

@Temperature 23.0 °C
5.25 - 5.99 ft-lb/in

@Temperature 73.4 °F
ISO R180
Fainplast Compounds RH 206/C Rigid PVC, Antishock Extrusion
Medium antishock profiles
Izod Impact, Unnotched 2.80 - 3.20 J/cm

@Temperature 23.0 °C
5.25 - 5.99 ft-lb/in

@Temperature 73.4 °F
ISO R180
Fainplast Compounds RH 612 Rigid PVC, Antishock Extrusion
Medium antishock profiles
Izod Impact, Unnotched 2.80 - 3.20 J/cm

@Temperature 23.0 °C
5.25 - 5.99 ft-lb/in

@Temperature 73.4 °F
ISO R180
Fainplast Compounds RKS 311 Rigid PVC, Antishock Extrusion Lead Free
Antishock profiles
Izod Impact, Unnotched 2.80 J/cm

@Thickness 3.20 mm,
Temperature 23.0 °C
5.25 ft-lb/in

@Thickness 0.126 in,
Temperature 73.4 °F
ASTM D256
Kingfa JH-R2G10 P60 10% Glass Fiber Reinforced PC/ABS Alloy
Features:UL HB @ 1.6-3.2mmExcellent balance propertiesHigh stiffnessGood size stabilityGood surface adhesionExcellent processing properties, large partsApplications:Injection moldingAutomobile instr..
Izod Impact, Unnotched 2.80 J/cm
5.25 ft-lb/in
ASTM D4812
SABIC Innovative Plastics Valox® DR48 PBT (Europe-Africa-Middle East)
VALOX DR48 is a 17% glass reinforced, flame retardant injection moulding PBT resin. Applications: lamp sockets, connectors, switches, electrical housings and bases, bobbins, trimmers and electromoto..
Izod Impact, Unnotched 2.80 J/cm

@Temperature -30.0 °C
5.25 ft-lb/in

@Temperature -22.0 °F
ASTM D4812
SABIC Innovative Plastics Valox® ENH8530 PBT+PET (Europe-Africa-Middle East)
Non-Brominated & Non-Chlorinated Flame Retardant, 15% Glass fiber reinforced PBT/PET blend
Izod Impact, Unnotched 2.80 J/cm
5.25 ft-lb/in
ASTM D256
Styrolution NAS® 90 High Performance Styrenic
NAS® 90 has sparkling clarity, improved toughness, and good scratch resistance. This easily processed copolymer blends well with clear impact modifiers. It meets USP XXIII Spec. of Class VI Pla..
Izod Impact, Unnotched 2.80 J/cm
5.25 ft-lb/in
ASTM D256
Solvay Specialty Polymers Ixef® 2530/X9027 Polyarylamide, 55% Mineral + Glass Fiber, at Equilibrium (65% RH)  
The IXEF compounds are a family of semi-crystalline polyarylamide thermoplastics reinforced with glass fibers and/or mineral fillers for injection molding.Data provided by the manufacturer, Solvay A..
Izod Impact, Unnotched 2.80 - 7.45 J/cm

@Temperature -30.0 - -30.0 °C
5.25 - 14.0 ft-lb/in

@Temperature -22.0 - -22.0 °F
Average value: 4.67 J/cm Grade Count:8
Overview of materials for PBT + PET Blend, Glass Filled